Mechanical Properties Metric English Comments
Tensile Strength, Yield 8.50 MPa

@Strain 100 %
1230 psi

@Strain 100 %
ASTM D-412
BASF Elastollan® M85A55 Polyester Type Polyurethane Elastomer
The Elastollan M Series of products listed are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are specifically formulated for fast cycling in Injection Molding appl..
Tensile Strength, Yield 8.50 MPa

@Strain 5.00 %
1230 psi

@Strain 5.00 %
ISO 527-1/-2
DSM Arnitel® PB581-H Polyether Ester Elastomer (European Grade)  (discontinued **)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..