Polymer Property : Tensile Strength, Yield = 116000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 800 MPa

@Temperature 23.9 °C
116000 psi

@Temperature 75.0 °F
0° Direction, Dry; ASTM D3039
Park Electrochemical Nelcote® E-718 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-718 is a modified epoxy resin system. E-718 is designed to provide excellent mechanical properties at low cure pressures.Key Features and Benefits:Good low pressure consolidationExcellen..
Tensile Strength, Yield >= 800 MPa

@Thickness 65.0 mm
>= 116000 psi

@Thickness 2.56 in
ThyssenKrupp N-A-XTRA® 800 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied with a minimum yield strength of 800 MPa. It can ..
Tensile Strength, Yield >= 800 MPa

@Thickness 65.0 mm
>= 116000 psi

@Thickness 2.56 in
ThyssenKrupp N-A-XTRA® M 800 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied with a minimum yield strength of 800 MPa. It can ..
Tensile Strength, Yield 800 MPa

@Strain 0.200 %
116000 psi

@Strain 0.200 %
hardened
Wieland Simidur KF Plus PFM Alloy
Palladium-base ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneeringDental
Tensile Strength, Yield 800 MPa

@Temperature 90.6 °C
116000 psi

@Temperature 195 °F
0°, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber
Information provided by HexCel
Tensile Strength, Yield 800 MPa

@Temperature 25.0 °C
116000 psi

@Temperature 77.0 °F
90°, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, A280-5H Fiber
Information provided by HexCel
Tensile Strength, Yield 800 MPa

@Temperature 20.0 °C
116000 psi

@Temperature 68.0 °F
Round bar 1" diameter, 310 HB
EDRO #2 Prehardened 4130 Holder Block
EDRO #2™ is a vacuum-degassed Chromium-Molybdenum-alloyed steel which is supplied in the hardened and tempered condition. EDRO #2™ is characterized by excellent machinability, good resistance to i..
Tensile Strength, Yield 800 MPa

@Temperature 20.0 °C
116000 psi

@Temperature 68.0 °F
Round bar 1" diameter, 310 HB
EDRO #3 Prehardened Mold Quality P20 Alloy Steel
EDRO #3™ is a vacuum-degassed, ladle refined, Cr-Ni-Mo- alloyed steel which is supplied in the hardened and tempered condition. EDRO #3™ is manufactured to consistently high quality standards with..
Tensile Strength, Yield 800 MPa

@Strain 0.200 %
116000 psi

@Strain 0.200 %
Double Age
Crucible Compaction Metals P/M 625 Corrosion Resistant Alloy
P/M 625 (chemically, UNS N06625) is produced by the Crucible P/M process: inert gas atomization, coupled with consolidation by hot isostatic pressing (HIP) and/or extrusion. The Crucible powder con..