Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 16.1 x 10-8 mm³/N-M | 8.00 x 10-10 in³-min/ft-lb-hr | Ring; ASTM D 3702 Modified |
SABIC Innovative Plastics LNP Lubricomp DFP22H PC LNP* Lubricomp* DFP22H is a compound based on Polycarbonate containing Glass Fiber and PTFE. Characteristics of this grade are: Internally Lubricated and Healthcare.This data was supplied by SABIC.. |
|||
K (wear) Factor | 16.1 - 806 x 10-8 mm³/N-M | 8.00 - 400 x 10-10 in³-min/ft-lb-hr | Average value: 86.1 x 10<sup>-8</sup> mm³/N-M Grade Count:30 |
Overview of materials for Acetal Copolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of.. |
|||
K (wear) Factor | 16.1 - 38.3 x 10-8 mm³/N-M | 8.00 - 19.0 x 10-10 in³-min/ft-lb-hr | Average value: 31.3 x 10<sup>-8</sup> mm³/N-M Grade Count:11 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |
|||
K (wear) Factor | 16.1 x 10-8 mm³/N-M | 8.00 x 10-10 in³-min/ft-lb-hr | |
Greene Tweed Avalon® 87 PTFE, Glass Filled Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin.. |
|||
K (wear) Factor | 16.1 x 10-8 mm³/N-M | 8.00 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP DL0049EF PC LNP* Lubricomp* DL0049EF is a compound based on Polycarbonate resin containing 20% PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retardant |
|||
K (wear) Factor | 16.1 x 10-8 mm³/N-M | 8.00 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP DL0049EF PC (Asia Pacific) LNP* Lubricomp* DL0049EF is a compound based on Polycarbonate resin containing PTFE, Flame Retardant. Added features of this material include: Internally Lubricated. |
|||
K (wear) Factor | 16.1 x 10-8 mm³/N-M | 8.00 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP KA000 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KA000 is a compound based on Acetal Copolymer resin containing Aramid Fiber, Proprietary Lubricant. |
|||
K (wear) Factor | 16.1 x 10-8 mm³/N-M | 8.00 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP KAL22 Acetal Copolymer LNP* LUBRICOMP* KAL22 is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid Fiber. Added feature of this material is: Wear Resistant. |
|||
K (wear) Factor | 16.1 x 10-8 mm³/N-M | 8.00 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP KAL22 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KAL22 is a compound based on Acetal Copolymer resin containing PTFE, Aramid Fiber. |
|||
K (wear) Factor | 16.1 x 10-8 mm³/N-M | 8.00 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP KP002 Acetal Copoly LNP* LUBRICOMP* KP002 is a compound based on Acetal Copolymer resin containing 10% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
K (wear) Factor | 16.1 x 10-8 mm³/N-M | 8.00 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP KP002 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KP002 is a compound based on Acetal Copolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
K (wear) Factor | 16.1 x 10-8 mm³/N-M | 8.00 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP KX06415 Acetal Copolymer LNP LUBRICOMP* KX06415 is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid Powder. Added features of this material include: Easy Molding, Heat Stabilized, Wear Resistant. |
|||
K (wear) Factor | 16.1 x 10-8 mm³/N-M | 8.00 x 10-10 in³-min/ft-lb-hr | Ring; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RBL36XXJ PA 66 LNP* LUBRICOMP* RBL36XXJ is a compound based on Nylon 66 containing 30% Glass Bead, 15% PTFE. Added features of this grade include: Low Extractable, Healthcare, Wear Resistant. |
|||
K (wear) Factor | 16.1 x 10-8 mm³/N-M | 8.00 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRILOY RX05498 PA 66 LNP LUBRILOY* RX05498 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: High Impact, Wear Resistant. |
|||
K (wear) Factor | 16.1 x 10-8 mm³/N-M | 8.00 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRILOY RX05498 PA 66 (Asia Pacific) LNP LUBRILOY* RX05498 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: High Impact. |
|||
K (wear) Factor | 16.1 x 10-8 mm³/N-M | 8.00 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
K (wear) Factor | 16.1 x 10-8 mm³/N-M | 8.00 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 (Asia Pacific) LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
K (wear) Factor | 16.1 x 10-8 mm³/N-M | 8.00 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 (Europe-Africa-Middle East) LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
K (wear) Factor | 16.1 x 10-8 mm³/N-M | 8.00 x 10-10 in³-min/ft-lb-hr | |
Techmer ES Luriblend® PA6 CF30 TL15 BK 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant (15%)Features: Low Friction, Good Wear Resistance and LubricatedAppearance: .. |
|||
K (wear) Factor | 16.1 x 10-8 mm³/N-M | 8.00 x 10-10 in³-min/ft-lb-hr | |
Techmer ES Luriblend® PA6 CF30 TS15 BK 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant (15%) and Silicone LubricantFeatures: LubricatedAppearance: Natural ColorPro.. |
|||
K (wear) Factor | 16.1 x 10-8 mm³/N-M | 8.00 x 10-10 in³-min/ft-lb-hr | |
Techmer ES Luriblend® PA6/6 CF30 TL12 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE + Silicone Lubricant(15%)Features: Lubricated and Good Wear ResistanceTPCI# 6466101Inf.. |
|||
K (wear) Factor | 16.1 x 10-8 mm³/N-M | 8.00 x 10-10 in³-min/ft-lb-hr | |
Techmer ES Luriblend® PA6/6 CF30 TL15 BK 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%) Features: Lubricated, Good Wear Resistance and Low Friction Appearance.. |
|||
K (wear) Factor | 16.1 x 10-8 mm³/N-M | 8.00 x 10-10 in³-min/ft-lb-hr | |
Techmer ES Luriblend® PA6/6 CF30 TL15 HS BK 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%) and Heat StabilizerFeatures: Lubricated, Good Wear Resistance, Heat Sta.. |
|||
K (wear) Factor | 16.1 x 10-8 mm³/N-M | 8.00 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP KAL22M Acetal Copolymer LNP LUBRICOMP* KAL22M is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant. |