Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 153 x 10-8 mm³/N-M | 76.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP DFL34 PC LNP LUBRICOMP* DFL34 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
K (wear) Factor | 153 x 10-8 mm³/N-M | 76.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP DFL34H PC LNP LUBRICOMP* DFL34H is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Healthcare. |