Mechanical Properties Metric English Comments
K (wear) Factor 121 x 10-8 mm³/N-M
60.0 x 10-10 in³-min/ft-lb-hr
QTM 55010
Quadrant EPP Acetron® AF Blend POM-H Acetal Extruded PTFE-Filled Acetal Homopolymer (ASTM Product Data Sheet)
K (wear) Factor 121 x 10-8 mm³/N-M
60.0 x 10-10 in³-min/ft-lb-hr
QTM 55010
Quadrant EPP Ertalyte® PET-P, Polyester-semi-crystalline thermoplastic, extruded (ASTM Product Data Sheet)
K (wear) Factor 121 x 10-8 mm³/N-M
60.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP DL003 PC
LNP LUBRICOMP* DL003 is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Internally Lubricated.
K (wear) Factor 121 x 10-8 mm³/N-M
60.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP DL003 PC (Asia Pacific)
LNP LUBRICOMP* DL003 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated.
K (wear) Factor 121 x 10-8 mm³/N-M
60.0 x 10-10 in³-min/ft-lb-hr
QTM 55010
Technetics Group Amicon™ PET-P  (Unverified Data**)
Information provided by Technetics Group (formerly Plastomer Technologies)
K (wear) Factor 121 x 10-8 mm³/N-M
60.0 x 10-10 in³-min/ft-lb-hr
QTM 55010
Quadrant EPP Duratron® PBI CU60 Polybenzimidazole, unfilled, compression molded (ASTM Product Data Sheet)
Duratron® PBI is the highest performance engineering plastic available from Quadrant EPP. It offers the highest mechanical properties of any thermoplastic above 400° F (205° C). Duratron® PBI ..
K (wear) Factor 121 x 10-8 mm³/N-M
60.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP DL003E PC (Asia Pacific)
LNP LUBRICOMP* DL003E is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Easy Molding.
K (wear) Factor 121 x 10-8 mm³/N-M
60.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP DL003EU PC
LNP LUBRICOMP* DL003EU is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Easy Molding, UV Stabilized, Internally Lubricated.
K (wear) Factor 121 x 10-8 mm³/N-M
60.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP DL003P PC
LNP LUBRICOMP* DL003P is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Exceptional Processing, Internally Lubricated.
K (wear) Factor 121 x 10-8 mm³/N-M
60.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP DL003P PC (Asia Pacific)
LNP LUBRICOMP* DL003P is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Exceptional Processing.
K (wear) Factor 121 x 10-8 mm³/N-M
60.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP JFL36 PES
LNP LUBRICOMP* JFL36 is a compound based on Polyethersulfone resin containing 30% Glass Fiber, 15% PTFE. Added featurs of this material is: Wear Resistant.
K (wear) Factor 121 x 10-8 mm³/N-M
60.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP JFL36 PES (Asia Pacific)
LNP LUBRICOMP* JFL36 is a compound based on Polyethersulfone resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
K (wear) Factor 121 x 10-8 mm³/N-M
60.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP JFL36 PES (Europe-Africa-Middle East)
LNP* Lubricomp* JFL36 is a compound based on Polyethersulfone resin containing Glass Fiber, PTFE.
K (wear) Factor 121 x 10-8 mm³/N-M
60.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP OCL36EXP PPS - LINEAR
LNP* LUBRICOMP* OCL36EXP is a compound based on Linear PPS containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include; Wear Resistant, Electrically Conductive.
K (wear) Factor 121 x 10-8 mm³/N-M
60.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRILOY D2000 PC
LNP LUBRILOY* D2000 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
K (wear) Factor 121 x 10-8 mm³/N-M
60.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRILOY D2000 PC (Asia Pacific)
LNP LUBRILOY* D2000 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
K (wear) Factor 121 x 10-8 mm³/N-M
60.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRILOY D2000AXH PC
LNP LUBRILOY* D2000AXH is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare.
K (wear) Factor 121 x 10-8 mm³/N-M
60.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D 3702 Modified
SABIC Innovative Plastics LNP Lubriloy D2000XXH PC
LNP LUBRILOY* D2000XXH is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated, Healthcare.This data was supplied..
K (wear) Factor 121 x 10-8 mm³/N-M
60.0 x 10-10 in³-min/ft-lb-hr
Techmer ES Luriblend® TPX-HDPE-99018
Availability: North AmericaForms: Pellets)Features: Good Wear Resistance and Low FrictionProcessing Method: Injection MoldingTPCI# 8869115Information provided by TP Composites, Inc.
K (wear) Factor 121 x 10-8 mm³/N-M
60.0 x 10-10 in³-min/ft-lb-hr
Thrust washer at 2000 PV
Techmer ES Plaslube® J-3/30/TF/13/SI/2 Nylon 6, 30% GFR, 13% PTFE, 2% Silicone
Plaslube glass fiber reinforced polytetrafluoroethylene (PTFE) lubricated nylon 612 grades offer a unique balance of excellent wear and friction performance with good dimensional stability and mecha..
K (wear) Factor 121 x 10-8 mm³/N-M
60.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP DL003E PC
LNP LUBRICOMP* DL003E is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Easy Molding, Internally Lubricated
K (wear) Factor 121 x 10-8 mm³/N-M
60.0 x 10-10 in³-min/ft-lb-hr
40psi, 50ft/min; tested in accordance with LNP WI-0687
LNP Lubricomp® JFL-4036 Polyethersulfone, Glass Fiber Reinforcement, PTFE Lubricant  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..