Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 5840 x 10-8 mm³/N-M | 2900 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Quadrant EPP Duratron® PEI U1000 LSG Polyetherimide, unfilled, extruded, Biocompatibility tested (ASTM Product Data Sheet) Duratron® U1000 (Formerly Ultem® 1000) polyetherimide is an amorphous, high-performance polymer with exceptional flame and heat resistance. It performs continuously to 340°F (171°C), making it.. |
|||
K (wear) Factor | 5840 x 10-8 mm³/N-M | 2900 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Quadrant EPP Duratron® PEI U1000 Extruded Unfilled Polyetherimide (ASTM Product Data Sheet) |