Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 54.4 x 10-8 mm³/N-M | 27.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP DFL36ELH PC LNP* Lubricomp* DFL36ELH is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractible, Easy Moldi.. |
|||
K (wear) Factor | 54.4 x 10-8 mm³/N-M | 27.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP DFL36XXJ PC LNP* Lubricomp* DFL36XXJ is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractable, Healthcare.. |
|||
K (wear) Factor | 54.4 x 10-8 mm³/N-M | 27.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP DFL36ELH PC (Asia Pacific) LNP* Lubricomp* DFL36ELH is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
K (wear) Factor | 54.4 x 10-8 mm³/N-M | 27.0 x 10-10 in³-min/ft-lb-hr | PV=2000 psi-fpm vs Self; SABIC Method |
SABIC Innovative Plastics ULTEM 4001 PEI PTFE filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
K (wear) Factor | 54.4 x 10-8 mm³/N-M | 27.0 x 10-10 in³-min/ft-lb-hr | PV=2000 psi-fpm vs Self; SABIC Method |
SABIC Innovative Plastics ULTEM 4001 PEI (Asia Pacific) PTFE filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
K (wear) Factor | 54.4 x 10-8 mm³/N-M | 27.0 x 10-10 in³-min/ft-lb-hr | Ring; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRILOY DF206XXH PC LNP* LUBRILOY* DF206XXH is a compound based on Polycarbonate containing 30% Glass Fiber, Proprietary Lubricant. Added features of this grade include: Wear Resistant, Healthcare. |