Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 10100 x 10-8 mm³/N-M | 5000 x 10-10 in³-min/ft-lb-hr | Average value: 10100 x 10<sup>-8</sup> mm³/N-M Grade Count:3 |
Overview of materials for Polyphthalamide (PPA), Stainless Fiber, EMI This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum va.. |
|||
K (wear) Factor | 10100 x 10-8 mm³/N-M | 5000 x 10-10 in³-min/ft-lb-hr | Average value: 10100 x 10<sup>-8</sup> mm³/N-M Grade Count:3 |
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled". Each property range of values reported i.. |
|||
K (wear) Factor | 10100 x 10-8 mm³/N-M | 5000 x 10-10 in³-min/ft-lb-hr | Average value: 10100 x 10<sup>-8</sup> mm³/N-M Grade Count:3 |
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled". Each property range of values reported .. |
|||
K (wear) Factor | 10100 x 10-8 mm³/N-M | 5000 x 10-10 in³-min/ft-lb-hr | Average value: 10100 x 10<sup>-8</sup> mm³/N-M Grade Count:4 |
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
K (wear) Factor | 10100 x 10-8 mm³/N-M | 5000 x 10-10 in³-min/ft-lb-hr | Average value: 10100 x 10<sup>-8</sup> mm³/N-M Grade Count:4 |
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and .. |
|||
K (wear) Factor | 10100 x 10-8 mm³/N-M | 5000 x 10-10 in³-min/ft-lb-hr | Average value: 10100 x 10<sup>-8</sup> mm³/N-M Grade Count:3 |
Overview of materials for Polypropylene, Stainless Fiber, EMI This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu.. |
|||
K (wear) Factor | 10100 x 10-8 mm³/N-M | 5000 x 10-10 in³-min/ft-lb-hr | Average value: 10100 x 10<sup>-8</sup> mm³/N-M Grade Count:3 |
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi.. |
|||
K (wear) Factor | 10100 x 10-8 mm³/N-M | 5000 x 10-10 in³-min/ft-lb-hr | Average value: 10100 x 10<sup>-8</sup> mm³/N-M Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS), Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Stainless Steel Fiber". Each property range of values reported is minimum a.. |