Mechanical Properties Metric English Comments
K (wear) Factor 50.4 x 10-8 mm³/N-M
25.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT
LNP* Lubricomp* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Ret..
K (wear) Factor 50.4 x 10-8 mm³/N-M
25.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT (Asia Pacific)
LNP* Lubricomp* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Ret..
K (wear) Factor 50.4 x 10-8 mm³/N-M
25.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP WL002 PBT
LNP* LUBRICOMP WL002 is a compound based on PBT resin containing 10% PTFE. Added feature of this grade is: Wear Resistant.
K (wear) Factor 50.4 x 10-8 mm³/N-M
25.0 x 10-10 in³-min/ft-lb-hr
Thrust washer at 2000 PV
Techmer ES Plaslube® J-1/30/TF/10 Nylon 66, 30% GFR, 10% PTFE
Plaslube glass fiber reinforced, polytetrafluoroethylene (PTFE) lubricated nylon 66 grades offer an excellent balance of wear and friction performance and mechanical strength. The addition of silic..
K (wear) Factor 50.4 x 10-8 mm³/N-M
25.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP JCL36E PES
LNP* LUBRICOMP* JCL36E is a compound based on Polyethersulfone (PES) resin containing 30% Carbon Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant.
K (wear) Factor 50.4 x 10-8 mm³/N-M
25.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT
LNP* LUBRICOMP* WBL36L is a compound based on PBT resin containing 30% Glass Bead, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible.
K (wear) Factor 50.4 x 10-8 mm³/N-M
25.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT (Asia Pacific)
LNP* Lubricomp* WBL36L is a compound based on Polybutylene Terephalate resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
K (wear) Factor 50.4 x 10-8 mm³/N-M
25.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP WCL36 PBT
LNP* LUBRICOMP* WCL36 is a compound based on PBT resin containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include: Electrically Conductive, Wear Resistant.