Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 888 x 10-8 mm³/N-M | 441 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP DX00714H PC LNP LUBRICOMP* DX00714H is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Wear Resistant, Healthcare. |
|||
K (wear) Factor | 888 x 10-8 mm³/N-M | 441 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP DX00714H PC (Asia Pacific) LNP LUBRICOMP* DX00714H is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated. |