Mechanical Properties Metric English Comments
K (wear) Factor 866 x 10-8 mm³/N-M
430 x 10-10 in³-min/ft-lb-hr
PV=2000 psi-fpm vs Self; SABIC Method
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C2801 PC+ABS
LNP* Lubricomp* Cycoloy_C2801 compound is a 5% PTFE reinforced PC+ABS, wear resistant, flame retardant compound for moving components in business equipment. Medium heat performance
K (wear) Factor 866 x 10-8 mm³/N-M
430 x 10-10 in³-min/ft-lb-hr
PV=2000 psi-fpm vs Self; SABIC Method
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C2801 PC+ABS (Asia Pacific)
5% PTFE reinforced PC+ABS wear resistant flame retardant resin for moving components in business equipment. Medium heat performance
K (wear) Factor 866 x 10-8 mm³/N-M
430 x 10-10 in³-min/ft-lb-hr
PV=2000 psi-fpm vs Self; SABIC Method
SABIC Innovative Plastics Cycoloy® C2805 PC+ABS
LNP* Lubricomp* Cycoloy* C2805 compound is a PTFE reinforced PC+ABS, wear resistant, flame retardant compound for moving components in business equipment. Medium heat performance
K (wear) Factor 866 x 10-8 mm³/N-M
430 x 10-10 in³-min/ft-lb-hr
PV=2000 psi-fpm vs Self; SABIC Method
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C2801 PC+ABS (Europe-Africa-Middle East)
LNP* Lubricomp* Cycoloy_C2801 compound is a 5% PTFE reinforced PC+ABS wear resistant flame retardant resin for moving components in business equipment. Medium heat performance
K (wear) Factor 866 x 10-8 mm³/N-M
430 x 10-10 in³-min/ft-lb-hr
PV=2000 psi-fpm vs Self; SABIC Method
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C2801R PC+ABS
LNP* Lubricomp* Cycoloy_C2801R compound is a 5% PTFE reinforced PC+ABS wear resistant, flame retardant compound for moving components in business equipment. 30% recycle content.