Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 423 x 10-8 mm³/N-M | 210 x 10-10 in³-min/ft-lb-hr | 40 psi, 50 fpm; ASTM D3702 |
Ensinger ENSITEP® PET Polyethylene Terephthalate - Extruded Products
(discontinued **) ENSITEP is an unreinforced, semi-crystalline thermoplastic polyester derived from polyethylene terephthalate. Its excellent wear resistance, low coefficient of friction, high flexural modulus, and .. |