Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 34.2 x 10-8 mm³/N-M | 17.0 x 10-10 in³-min/ft-lb-hr | Dry: 4 m/s, 0.2 MPa (800 fpm, 31.25 psi); ASTM D3702 |
Solvay Specialty Polymers Torlon® 4301 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4301 is a wear-resistant grade of polyamide-imide (PAI) resin. It has a good balance of mechanical properties and wear resistance. It offers high flexural and compressive strength with a low .. |
|||
K (wear) Factor | 34.2 x 10-8 mm³/N-M | 17.0 x 10-10 in³-min/ft-lb-hr | Dry: 4 m/s, 0.2 MPa (800 fpm, 31.25 psi); ASTM D3702 |
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not only.. |
|||
K (wear) Factor | 34.2 x 10-8 mm³/N-M | 17.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RX05487 PA 66 LNP* LUBRICOMP* RX05487 is a compound based on Nylon 66 containing 10% Aramid Fiber, 10% Lubricant. Added features of this material are: Low Warpage, Wear Resistant. |
|||
K (wear) Factor | 34.2 x 10-8 mm³/N-M | 17.0 x 10-10 in³-min/ft-lb-hr | |
Techmer ES Luriblend® PA6 GF30 TL15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightAdditive: Heat Stabilized and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Heat Stab.. |