Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 320 x 10-8 mm³/N-M | 159 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RFN16S PA 66 LNP LUBRICOMP* RFN16S is a compound based on Nylon 66 resin containing 30% Glass Fiber, 5% MOS2. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
K (wear) Factor | 320 x 10-8 mm³/N-M | 159 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D 3702 Modified |
SABIC Innovative Plastics LNP Lubricomp RFN16SXS PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFN16SXS is a compound based on Nylon 66 resin containing Glass Fiber, MOS2. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Euro.. |
|||
K (wear) Factor | 320 x 10-8 mm³/N-M | 159 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RFN16SXZ PA 66 LNP LUBRICOMP* RFN16SXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber, 5% MOS2. Added features of this material include: Heat Stabilized, Wear Resistant. |