Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 26.2 x 10-8 mm³/N-M | 13.0 x 10-10 in³-min/ft-lb-hr | 40psi, 50ft/min; tested in accordance with LNP WI-0687 |
LNP Lubricomp® LCL-4033 EM Polyetheretherketone, Carbon Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: Good Moldability, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP g.. |
|||
K (wear) Factor | 26.2 x 10-8 mm³/N-M | 13.0 x 10-10 in³-min/ft-lb-hr | Ring; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP DFL34EH PC LNP* LUBRICOMP* DFL34EH is a compound based on Polycarbonate containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Easy Molding, Healthcare, Wear Resistant. |
|||
K (wear) Factor | 26.2 x 10-8 mm³/N-M | 13.0 x 10-10 in³-min/ft-lb-hr | Dry: 0.25 m/s, 3.4 MPa (50 fpm, 500 psi) |
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus with .. |
|||
K (wear) Factor | 26.2 x 10-8 mm³/N-M | 13.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP EX03647H PEI LNP LUBRICOMP* EX03647H is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Healthcare, Wear Resistant. |
|||
K (wear) Factor | 26.2 x 10-8 mm³/N-M | 13.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP IBP34 PA6.12 LNP* LUBRICOMP* IBP34 is a compound based on Nylon 6/12 containing 20% Glass Bead, 15% PTFE/Silicone. Added features include: Wear Resistant. |
|||
K (wear) Factor | 26.2 x 10-8 mm³/N-M | 13.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP LCL33 PEEK LNP* LUBRICOMP* LCL33 is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
K (wear) Factor | 26.2 x 10-8 mm³/N-M | 13.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP LCL33 PEEK (Europe-Africa-Middle East) LNP* LUBRICOMP* LCL33 is a compound based on Polyethereketone resin containg Carbon Fiber, PTFE. Added features include: Elecrtically Conductive , Internally Lubricated. |
|||
K (wear) Factor | 26.2 x 10-8 mm³/N-M | 13.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP LCL33E PEEK LNP LUBRICOMP* LCL33E is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Easy Molding, Wear Resistant. |
|||
K (wear) Factor | 26.2 x 10-8 mm³/N-M | 13.0 x 10-10 in³-min/ft-lb-hr | Ring; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP ML004 PP LNP* LUBRICOMP* ML004 is a product based on Polypropylene containing 20% PTFE. Added features of this grade include: Wear Resistant. |
|||
K (wear) Factor | 26.2 x 10-8 mm³/N-M | 13.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RAL22 PA 66 LNP LUBRICOMP* RAL22 is a compound based on Nylon 66 resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant. |
|||
K (wear) Factor | 26.2 x 10-8 mm³/N-M | 13.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RAL22 PA 66 (Asia Pacific) LNP LUBRICOMP* RAL22 is a compound based on Nylon 66 resin containing Aramid, PTFE. Added features of this material include: Internally Lubricated. |
|||
K (wear) Factor | 26.2 x 10-8 mm³/N-M | 13.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RAL22 PA 66 (Europe-Africa-Middle East) LNP* LUBRICOMP* RAL22 is a compound based on PA66 resin containing PTFE, Aramid Fiber. Added Features: Internally Lubricated |
|||
K (wear) Factor | 26.2 x 10-8 mm³/N-M | 13.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RAL22S PA 66 LNP* LUBRICOMP* RAL22S is a compound based on Nylon 66 resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant. |
|||
K (wear) Factor | 26.2 x 10-8 mm³/N-M | 13.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RAL22S PA 66 (Asia Pacific) LNP* Lubricomp* RAL22S is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
K (wear) Factor | 26.2 x 10-8 mm³/N-M | 13.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12 LNP* LUBRICOMP* SP003 is a compound based on Nylon 12 resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
K (wear) Factor | 26.2 x 10-8 mm³/N-M | 13.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12 (Asia Pacific) LNP* Lubricomp* SP003 is a compound based on Nylon 12 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
K (wear) Factor | 26.2 x 10-8 mm³/N-M | 13.0 x 10-10 in³-min/ft-lb-hr | |
Techmer ES Luriblend® PA6/6 GF10 M/TL10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: Molybdenum Disulfide Lubricant and PTFE LubricantFeatures: LubricatedAppearance: Natural Col.. |