Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 24.2 x 10-8 mm³/N-M | 12.0 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Quadrant EPP Nylatron® NSM Nylon, Cast Solid Lubricant Filled, Type 6 (ASTM Product Data Sheet) |
|||
K (wear) Factor | 24.2 - 161 x 10-8 mm³/N-M | 12.0 - 80.0 x 10-10 in³-min/ft-lb-hr | Average value: 101 x 10<sup>-8</sup> mm³/N-M Grade Count:5 |
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v.. |
|||
K (wear) Factor | 24.2 x 10-8 mm³/N-M | 12.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP IFP36 PA6.12 LNP* LUBRICOMP* IFP36 is a Nylon 6/12 base resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features of t his grade include: Wear Resistant. |
|||
K (wear) Factor | 24.2 x 10-8 mm³/N-M | 12.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP KL004A Acetal Homopolymer LNP LUBRICOMP* KL004A is a compound based on Acetal Homopolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
K (wear) Factor | 24.2 x 10-8 mm³/N-M | 12.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP KL004A ACETAL HOMOPOLYMER (Europe-Africa-Middle East) LNP* LUBRICOMP* KL004A is a compound based on Acetal Homopolymer resin containing PTFE. Added features include: Internally Lubricated |
|||
K (wear) Factor | 24.2 x 10-8 mm³/N-M | 12.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP KL004AXC Acetal Homopolymer LNP* LUBRICOMP* KL004AXC is a compound based on Acetal Homopolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
K (wear) Factor | 24.2 x 10-8 mm³/N-M | 12.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP LX91475 PEEK (Asia Pacific) LNP* LUBRICOMP* LX91475 is a compound based on Polyetheretherketone resin containing Bearing Grade. Added features of this material include: Easy Molding. |
|||
K (wear) Factor | 24.2 x 10-8 mm³/N-M | 12.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RAL22I PA 66 LNP* LUBRICOMP* RAL22I is a compound based on Nylon 66 resin containing 10% PTFE, 10% Aramid Fiber. Added features of this material include: Wear Resistant, High Impact. |
|||
K (wear) Factor | 24.2 x 10-8 mm³/N-M | 12.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RFL16 PA 66 (Asia Pacific) LNP LUBRICOMP* RFL16 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
K (wear) Factor | 24.2 x 10-8 mm³/N-M | 12.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D 3702 Modified |
SABIC Innovative Plastics LNP Lubricomp RFL16S PA 66 LNP* Lubricomp* RFL16S is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Heat Stabilized.This data was supplied by .. |
|||
K (wear) Factor | 24.2 x 10-8 mm³/N-M | 12.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D 3702 Modified |
SABIC Innovative Plastics LNP Lubricomp RFL16S PA 66 (Asia Pacific) LNP* Lubricomp* RFL16S is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Heat Stabilized.This data was supplied by .. |
|||
K (wear) Factor | 24.2 x 10-8 mm³/N-M | 12.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RFL36S PA 66 LNP* LUBRICOMP* RFL36S is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
K (wear) Factor | 24.2 x 10-8 mm³/N-M | 12.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RFL36SXS PA 66 (Europe-Africa-Middle East) LNP* LUBRICOMP* RFL36SXS is a compound based on PA 66 resin containing Glass Fiber, PTFE. Added features include Internally Lubricated, Heat Stabilized. |
|||
K (wear) Factor | 24.2 x 10-8 mm³/N-M | 12.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RFL36XXY PA 66 LNP* LUBRICOMP* RFL36XXY is a compound based on Nylon 66 containing 30% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
K (wear) Factor | 24.2 x 10-8 mm³/N-M | 12.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RFL36XXZ PA 66 LNP* LUBRICOMP* RFL36XXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant. |
|||
K (wear) Factor | 24.2 x 10-8 mm³/N-M | 12.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RFL46ES PA 66 LNP* LUBRICOMP* RFL46ES is a compound based on Nylon 6/6 containing 30% Glass Fiber, 20% PTFE. Added features of this grade include: Wear Resistant, Heat Stabilized, Easy Molding. |
|||
K (wear) Factor | 24.2 x 10-8 mm³/N-M | 12.0 x 10-10 in³-min/ft-lb-hr | PV=2000 psi-fpm vs Self; SABIC Method |
SABIC Innovative Plastics ULTEM 4000 PEI (Europe-Africa-Middle East) Glass fiber, PTFE, and Graphite filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 listing. |
|||
K (wear) Factor | 24.2 x 10-8 mm³/N-M | 12.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRILOY KL201 Acetal LNP LUBRILOY* KL201 is a compound based on Acetal resin containing Proprietary Lubricant. PTFE. Added feature of this material is: Wear Resistant. |
|||
K (wear) Factor | 24.2 x 10-8 mm³/N-M | 12.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRILOY KL201 Acetal (Asia Pacific) LNP LUBRILOY* KL201 is a compound based on Acetal resin containing PTFE, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
K (wear) Factor | 24.2 x 10-8 mm³/N-M | 12.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRILOY KL201 Acetal (Europe-Africa-Middle East) LNP LUBRILOY* KL201 is a compound based on Acetal resin containing PTFE, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
K (wear) Factor | 24.2 x 10-8 mm³/N-M | 12.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRILOY R2000A PA 66 LNP LUBRILOY* R2000A is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
K (wear) Factor | 24.2 x 10-8 mm³/N-M | 12.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRILOY R2000A PA 66 (Asia Pacific) LNP LUBRILOY* R2000A is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
K (wear) Factor | 24.2 x 10-8 mm³/N-M | 12.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRILOY R2000A PA 66 (Europe-Africa-Middle East) LNP LUBRILOY* R2000A is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
K (wear) Factor | 24.2 x 10-8 mm³/N-M | 12.0 x 10-10 in³-min/ft-lb-hr | |
Techmer ES Luriblend® PA6/6 TL20 HS L Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant(20%)Features: Lubricated, Heat Stabilized and Good Wear ResistanceInformation provided by TP Composites, Inc. |
|||
K (wear) Factor | 24.2 x 10-8 mm³/N-M | 12.0 x 10-10 in³-min/ft-lb-hr | |
Techmer ES Luriblend® PA6/6 TS15 BK Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Lubricated, Heat Stabilized and Good Wear ResistanceAppearance: BlackInformation provided by TP Composites, .. |
|||
K (wear) Factor | 24.2 x 10-8 mm³/N-M | 12.0 x 10-10 in³-min/ft-lb-hr | |
Techmer ES Luriblend® PA6/6 TS20 HS Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilized, PTFE Lubricant(18%) and Silicone Lubricant (2%)Features: Lubricated, Good Wear Resistance and Heat StabilizedInformation provide.. |
|||
K (wear) Factor | 24.2 x 10-8 mm³/N-M | 12.0 x 10-10 in³-min/ft-lb-hr | ASTM D3702 |
Teknor Apex Chemlon® ALF20 Nylon 66, Unreinforced Notes: ALF20 is a self-lubricating grade of nylon 66 containing PTFE and Silicone. It offers outstanding surface wear characteristics of molded parts. It is suitable for applications such as beari.. |
|||
K (wear) Factor | 24.2 - 5840 x 10-8 mm³/N-M | 12.0 - 2900 x 10-10 in³-min/ft-lb-hr | Average value: 508 x 10<sup>-8</sup> mm³/N-M Grade Count:47 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |