Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 195 x 10-8 mm³/N-M | 97.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP DL002 PC (Europe-Africa-Middle East) LNP* Lubricomp* DL002 is a compound based on Polycarbonate resin containing PTFE. Added features include: Internally Lubricated. |
|||
K (wear) Factor | 195 x 10-8 mm³/N-M | 97.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP DL002P PC (Asia Pacific) LNP LUBRICOMP* DL002P is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Exceptional Processing. |
|||
K (wear) Factor | 195 x 10-8 mm³/N-M | 97.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP DL002PC PC LNP* LUBRICOMP* DL002PC is a compound based on Polycarbonate resin containing 10% PTFE. Added features of this grade are: Wear Resistant, Exceptional Processing, Clean Compound System. |
|||
K (wear) Factor | 195 x 10-8 mm³/N-M | 97.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP DL002 PC LNP LUBRICOMP* DL002 is a compound based on Polycarbonate resin containing 10% PTFE. Added features of this material include: Internally Lubricated. |
|||
K (wear) Factor | 195 x 10-8 mm³/N-M | 97.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP DL002 PC (Asia Pacific) LNP LUBRICOMP* DL002 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
K (wear) Factor | 195 x 10-8 mm³/N-M | 97.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP DL002P PC LNP LUBRICOMP* DL002P is a compound based on Polycarbonate resin containing 10% PTFE. Added features of this material include: Exceptional Processing, Internally Lubricated. |