Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : K (wear) Factor = 16.1 x 10-8 mm³/N-M Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 16.1 x 10-8 mm³/N-M
8.00 x 10-10 in³-min/ft-lb-hr
Ring; ASTM D 3702 Modified
SABIC Innovative Plastics LNP Lubricomp DFP22H PC
LNP* Lubricomp* DFP22H is a compound based on Polycarbonate containing Glass Fiber and PTFE. Characteristics of this grade are: Internally Lubricated and Healthcare.This data was supplied by SABIC..
K (wear) Factor 16.1 - 806 x 10-8 mm³/N-M
8.00 - 400 x 10-10 in³-min/ft-lb-hr
Average value: 86.1 x 10<sup>-8</sup> mm³/N-M Grade Count:30
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
K (wear) Factor 16.1 - 38.3 x 10-8 mm³/N-M
8.00 - 19.0 x 10-10 in³-min/ft-lb-hr
Average value: 31.3 x 10<sup>-8</sup> mm³/N-M Grade Count:11
Overview of materials for Nylon 66, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr..
K (wear) Factor 16.1 x 10-8 mm³/N-M
8.00 x 10-10 in³-min/ft-lb-hr
Greene Tweed Avalon® 87 PTFE, Glass Filled
Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin..
K (wear) Factor 16.1 x 10-8 mm³/N-M
8.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP DL0049EF PC
LNP* Lubricomp* DL0049EF is a compound based on Polycarbonate resin containing 20% PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retardant
K (wear) Factor 16.1 x 10-8 mm³/N-M
8.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP DL0049EF PC (Asia Pacific)
LNP* Lubricomp* DL0049EF is a compound based on Polycarbonate resin containing PTFE, Flame Retardant. Added features of this material include: Internally Lubricated.
K (wear) Factor 16.1 x 10-8 mm³/N-M
8.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP KA000 Acetal Copolymer (Europe-Africa-Middle East)
LNP* Lubricomp* KA000 is a compound based on Acetal Copolymer resin containing Aramid Fiber, Proprietary Lubricant.
K (wear) Factor 16.1 x 10-8 mm³/N-M
8.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP KAL22 Acetal Copolymer
LNP* LUBRICOMP* KAL22 is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid Fiber. Added feature of this material is: Wear Resistant.
K (wear) Factor 16.1 x 10-8 mm³/N-M
8.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP KAL22 Acetal Copolymer (Europe-Africa-Middle East)
LNP* Lubricomp* KAL22 is a compound based on Acetal Copolymer resin containing PTFE, Aramid Fiber.
K (wear) Factor 16.1 x 10-8 mm³/N-M
8.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP KP002 Acetal Copoly
LNP* LUBRICOMP* KP002 is a compound based on Acetal Copolymer resin containing 10% PTFE/Silicone. Added feature of this material is: Wear Resistant.
K (wear) Factor 16.1 x 10-8 mm³/N-M
8.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP KP002 Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KP002 is a compound based on Acetal Copolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.
K (wear) Factor 16.1 x 10-8 mm³/N-M
8.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP KX06415 Acetal Copolymer
LNP LUBRICOMP* KX06415 is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid Powder. Added features of this material include: Easy Molding, Heat Stabilized, Wear Resistant.
K (wear) Factor 16.1 x 10-8 mm³/N-M
8.00 x 10-10 in³-min/ft-lb-hr
Ring; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP RBL36XXJ PA 66
LNP* LUBRICOMP* RBL36XXJ is a compound based on Nylon 66 containing 30% Glass Bead, 15% PTFE. Added features of this grade include: Low Extractable, Healthcare, Wear Resistant.
K (wear) Factor 16.1 x 10-8 mm³/N-M
8.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRILOY RX05498 PA 66
LNP LUBRILOY* RX05498 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: High Impact, Wear Resistant.
K (wear) Factor 16.1 x 10-8 mm³/N-M
8.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRILOY RX05498 PA 66 (Asia Pacific)
LNP LUBRILOY* RX05498 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: High Impact.
K (wear) Factor 16.1 x 10-8 mm³/N-M
8.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66
LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
K (wear) Factor 16.1 x 10-8 mm³/N-M
8.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 (Asia Pacific)
LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
K (wear) Factor 16.1 x 10-8 mm³/N-M
8.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 (Europe-Africa-Middle East)
LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
K (wear) Factor 16.1 x 10-8 mm³/N-M
8.00 x 10-10 in³-min/ft-lb-hr
Techmer ES Luriblend® PA6 CF30 TL15 BK 30% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant (15%)Features: Low Friction, Good Wear Resistance and LubricatedAppearance: ..
K (wear) Factor 16.1 x 10-8 mm³/N-M
8.00 x 10-10 in³-min/ft-lb-hr
Techmer ES Luriblend® PA6 CF30 TS15 BK 30% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant (15%) and Silicone LubricantFeatures: LubricatedAppearance: Natural ColorPro..
K (wear) Factor 16.1 x 10-8 mm³/N-M
8.00 x 10-10 in³-min/ft-lb-hr
Techmer ES Luriblend® PA6/6 CF30 TL12 30% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE + Silicone Lubricant(15%)Features: Lubricated and Good Wear ResistanceTPCI# 6466101Inf..
K (wear) Factor 16.1 x 10-8 mm³/N-M
8.00 x 10-10 in³-min/ft-lb-hr
Techmer ES Luriblend® PA6/6 CF30 TL15 BK 30% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%) Features: Lubricated, Good Wear Resistance and Low Friction Appearance..
K (wear) Factor 16.1 x 10-8 mm³/N-M
8.00 x 10-10 in³-min/ft-lb-hr
Techmer ES Luriblend® PA6/6 CF30 TL15 HS BK 30% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%) and Heat StabilizerFeatures: Lubricated, Good Wear Resistance, Heat Sta..
K (wear) Factor 16.1 x 10-8 mm³/N-M
8.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP KAL22M Acetal Copolymer
LNP LUBRICOMP* KAL22M is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant.