Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 131 x 10-8 mm³/N-M | 65.0 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Quadrant EPP Nylatron® GSM Blue Nylon, Cast Oil & MoS2 Filled Type 6 (ASTM Product Data Sheet) |
|||
K (wear) Factor | 131 x 10-8 mm³/N-M | 65.0 x 10-10 in³-min/ft-lb-hr | ASTM G77 |
Greene Tweed Arlon® 1555 PEEK, Carbon, Graphite Filled Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie.. |
|||
K (wear) Factor | 131 x 10-8 mm³/N-M | 65.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRILOY ZX06315 PPE+SEBS+Polyolefin (Asia Pacific) LNP* Lubriloy* ZX06315 is a compound based on PPE+PS Blend resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Internally Lubricated, Non-Brominated & N.. |
|||
K (wear) Factor | 131 x 10-8 mm³/N-M | 65.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRILOY ZX06315 PPE+SEBS+Polyolefin (Europe-Africa-Middle East) LNP* Lubriloy* ZX06315 is a compound based on PPE+PS Blend resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Internally Lubricated, Non-Brominated & N.. |
|||
K (wear) Factor | 131 x 10-8 mm³/N-M | 65.0 x 10-10 in³-min/ft-lb-hr | 40 psi, 50 fpm |
Ensinger Tecaform™ AH ID Metal Detectable Acetal Copolymer (POM) TECAFORM™ AH ID is the fist commercially available acetal that is fully detectable by standard metal detection equipment. Exhibiting excellent machinability and a good combination of physical prop.. |
|||
K (wear) Factor | 131 x 10-8 mm³/N-M | 65.0 x 10-10 in³-min/ft-lb-hr | 40 psi, 50 fpm; ASTM D3702 |
Ensinger Tecaform™ Acetal Copolymer - Extruded Products (POM) Tecaform™ is a semi-crystalline thermoplastic offering high strength, stiffness and toughness. It is resistant to hot water, hydrocarbons and solvents, and it posses good bearing and wear properti.. |
|||
K (wear) Factor | 131 x 10-8 mm³/N-M | 65.0 x 10-10 in³-min/ft-lb-hr | vs steel; 40 psi, 50 fpm; ASTM D3702 |
Ensinger Tecaform™ FG Blue Food Grade Acetal (POM) Tecaform™ is resistant to hot water and typical cleaning chemicals. It possesses good bearing and wear properties. The blue color makes it more visible than standard grades. It is commonly used .. |