Polymer Property : K (wear) Factor = 12.9 x 10-10 in³-min/ft-lb-hr Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 26.0 x 10-8 mm³/N-M
12.9 x 10-10 in³-min/ft-lb-hr
3.4 MPa, 0.25 m/sec; ASTM D3702
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI)
Torlon® 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus w..