Polymer Property : K (wear) Factor = 10.1 x 10-8 mm³/N-M Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 10.1 - 30.2 x 10-8 mm³/N-M
5.00 - 15.0 x 10-10 in³-min/ft-lb-hr
Average value: 16.3 x 10<sup>-8</sup> mm³/N-M Grade Count:10
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value..
K (wear) Factor 10.1 x 10-8 mm³/N-M
5.00 x 10-10 in³-min/ft-lb-hr
Ring; ASTM D 3702 Modified
SABIC Innovative Plastics LNP Lubricomp KZL34 POM
LNP* Lubricomp* KZL34 is a compound based on Acetal resin containing Milled Glass and PTFE. Characteristic of this grade is Internally Lubricated.This data was supplied by SABIC-IP for the Americas..
K (wear) Factor 10.1 x 10-8 mm³/N-M
5.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP RFL26S PA 66
LNP* LUBRICOMP* RFL26S is a compound based on Nylon 66 resin containing 30% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Heat Stabilized.
K (wear) Factor 10.1 x 10-8 mm³/N-M
5.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP RFL26S PA 66 (Asia Pacific)
LNP* Lubricomp* RFL26S is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Heat Stabilized.
K (wear) Factor 10.1 x 10-8 mm³/N-M
5.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP RFL36U PA 66
LNP* LUBRICOMP* RFL36U is a compound based on Nylon 66 resin containing 15% PTFE, 30% Glass Fiber. Added features of this grade include: Wear Resistant, UV Stabilized.
K (wear) Factor 10.1 x 10-8 mm³/N-M
5.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP UFL36AS PPA
LNP* LUBRICOMP* UFL36AS is a Polyphthalamide (PPA) base resin containing 30% Glass Fiber, 15% PTFE. Added features of this material are: Heat Stabilized, Wear Resistant.
K (wear) Factor 10.1 x 10-8 mm³/N-M
5.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP UFL36AS PPA (Europe-Africa-Middle East)
LNP* LUBRICOMP* UFL36AS is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features include Internally Lubricated, Heat Stabilized.
K (wear) Factor 10.1 x 10-8 mm³/N-M
5.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D 3702 Modified
SABIC Innovative Plastics LNP Lubricomp UFL36ASP PPA (Europe-Africa-Middle East)
LNP* LUBRICOMP* UFL36ASP is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features include Internally Lubricated, Heat Stabilized.This data was supplied by SABIC-IP f..
K (wear) Factor 10.1 x 10-8 mm³/N-M
5.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP WX07423H PBT
Health care grade, PTFE and silicone lubricated
K (wear) Factor 10.1 x 10-8 mm³/N-M
5.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP YP003 POLYESTER ELASTOMER
LNP LUBRICOMP* YP003 is a compound based on Polyester Elastomer resin containing 15% PTFE/Silicone. Added features of this material include: Wear Resistant.
K (wear) Factor 10.1 x 10-8 mm³/N-M
5.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D 3702 Modified
SABIC Innovative Plastics LNP Lubricomp YP003 TPEE
LNP LUBRICOMP* YP003 is a compound based on TPEE resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas ..
K (wear) Factor 10.1 x 10-8 mm³/N-M
5.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRILOY RA2 PA 66
LNP* LUBRILOY* RA2 is a compound based on Nylon 66 resin containing Aramid Fiber. Added feature of this material is: Wear Resistant.
K (wear) Factor 10.1 x 10-8 mm³/N-M
5.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRILOY UA200A PPA
LNP LUBRILOY* UA200A is a compound based on Polyphthalamide resin containing Aramid Fiber, Proprietary Lubricant. Added feature of this material is: Wear Resistant.
K (wear) Factor 10.1 x 10-8 mm³/N-M
5.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRILOY UA200A PPA (Asia Pacific)
LNP LUBRILOY* UA200A is a compound based on Polyphthalamide resin containing Aramid Fiber, Proprietary Lubricant. Added features of this material include: Internally Lubricated.
K (wear) Factor 10.1 x 10-8 mm³/N-M
5.00 x 10-10 in³-min/ft-lb-hr
Ring; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP QFL32 PA 6/10
LNP* LUBRICOMP* QFL32 is a compound based on Nylon 6/10 containing 10% Glass Fiber, 15% PTFE. Added features of this grade include: Wear Resistant.