Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 1500 MPa
218000 psi
ASTM D790A
SABIC PP 412MK49 Polypropylene Impact Copolymer for Injection Molding
Product Description: PP 412MK49 is specially developed for producing injection molded articles. This grade contains an antistatic & nucleating agents. It has medium flow properties, good impact r..
Flexural Modulus, 1% Secant 1500 MPa
218000 psi
ASTM D790A
SABIC PP 49MK45 Polypropylene Impact Copolymer for Injection Molding
Product Description: PP 49MK45 is specially developed for producing injection molded articles. This grade contains an antistatic & nucleating agents. It has medium flow properties, good impact re..
Flexural Modulus, 1% Secant 1500 MPa
218000 psi
ASTM D790A
SABIC PP 500P Polypropylene Homopolymer for Raffia Applications
Product Description: PP 500P is specially developed for producing stretched tapes with the following features:Consistent processabilityEasy orientationLow water carry overGood mechanical properties..
Flexural Modulus, 1% Secant 1500 MPa
218000 psi
ASTM D790A
SABIC PP 506P Polypropylene Homopolymer for Raffia Applications
Product Description: PP 506P is intended for producing low denier stretched tapes with the following features:Consistent processabilityGood processability at high line speeds and low deniersLow tap..
Flexural Modulus, 1% Secant 1500 MPa
218000 psi
ASTM D790A
SABIC PP 519A Polypropylene Homopolymer for Spunbond Applications
Product Description: PP 519A is a controlled rheology grade with a narrow molecular weight distribution intended for spun bond fiber extrusion applications.PP 519A has the following features:Consis..
Flexural Modulus, 1% Secant 1500 MPa
218000 psi
ASTM D790A
SABIC PP 521P Polypropylene Homopolymer for Bi-axially Oriented Film
Product Description: PP 521P is a non formulated grade, specially developed for bi-axially oriented PP (BOPP) film extrusion with a very specific molecular structure providing ultimate properties r..
Flexural Modulus, 1% Secant 1500 MPa
218000 psi
ASTM D790A
SABIC PP 523P Polypropylene Homopolymer for Bi-axially Oriented Film
Product Description: PP 523P is a non formulated grade, specially developed for bi-axially oriented PP (BOPP) film extrusion with a very specific molecular structure providing ultimate properties r..
Flexural Modulus, 1% Secant 1500 MPa
218000 psi
ASTM D790A
Braskem H 155 Fiber Extrusion Polypropylene Homopolymer
Meltblown nonwoven applications for hygienic, medical and hospital disposable devices; Filters and oil adsorbents.Information provided by Braskem.
Flexural Modulus, 1% Secant 1500 MPa
218000 psi
ASTM-D790
Braskem PH 1721 HOMO Polypropylene Homopolymer
PH 1721 is a low melt flow rate polypropylene with an anti-gas fading stabilization package. It is suitable for continuous filament and staple fiber processing due to its molecular weight distributi..
Flexural Modulus, 1% Secant 1500 MPa
218000 psi
ASTM D790A
Braskem CP 405XP Compression Molding Polypropylene Heterophasic Copolymer
Bottle caps for carbonated beverages.Information provided by Braskem.
Flexural Modulus, 1% Secant 1500 MPa
218000 psi
0.05 in/min test speed
Ineos H19G-00 Polypropylene Homopolymer
This is a homopolymer designed for extrusion processing and meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsContinuous Filament YarnBCFSta..