Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 1380 MPa
200000 psi
0.5 in/min; ASTM D790B
ExxonMobil PP7654KNE2 Polypropylene Homopolymer
Product Description: A high impact copolymer resin with medium melt flow rate and excellent processing attributes. It is designed for injection molded large consumer and industrial parts.Availabili..
Flexural Modulus, 1% Secant 1380 MPa
200000 psi
ASTM D790A
Dow 5E89 Polypropylene Homopolymer Resin
OverviewConsistent processabilityGood color stabilityHigh strength propertiesLow water "carry-over"High speed processingComplies with U.S. FDA 21 CFR 177.1520 (c)1.1aDOW 5E89 Polypropylene Resin is ..
Flexural Modulus, 1% Secant 1380 MPa
200000 psi
ASTM D790A
Dow C758-80NA Polypropylene Impact Copolymer Resin
OverviewVery easy mold filling and fast set upGood balance of impact strength and stiffnessContains a nucleating and antistatic additiveComplies with: U.S. FDA FCN 843, Canadian HPFB No ObjectionDOW..
Flexural Modulus, 1% Secant 1380 MPa
200000 psi
ASTM D790A
Dow C759-21NA Polypropylene Impact Copolymer Resin
DOW C759-21NA Polypropylene Resin is an impact copolymer designed for injection molding with high stiffness, good impact resistance, and good antistatic properties. Key applications include foldabl..
Flexural Modulus, 1% Secant 1380 MPa
200000 psi
ASTM D790A
Dow DX5E66 Polypropylene Homopolymer Resin
OverviewConsistent processabilityVery high cleanlinessGood optical propertiesComplies with U.S. FDA 21 CFR 177.1520 (c)1.1a, EU-Directive 2002/72/EC, Canadian HPFB No ObjectionDX5E66 Developmental P..
Flexural Modulus, 1% Secant 1380 MPa
200000 psi
ASTM D790A
Dow NRD6-589 Polypropylene Random Copolymer Resin
DOW NRD6-589 Polypropylene Resin is intended for use in injection molding applications. It offers excellent balance of impact and stiffness.Consistent processabilityGood stiffness/impact balanceGoo..