Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1140 MPa | 165000 psi | ASTM D790 |
Flint Hills P5G2N-093 Random Copolymer Polypropylene Features: Nucleated. Product does not contain animal derived components.Applications: Compression molding, Caps and ClosuresInformation provided by Flint Hills Resources. |
|||
Flexural Modulus, 1% Secant | 1140 MPa | 165000 psi | ASTM D790A |
Dow 334.03 Developmental Performance Polypropylene Polymer DOW D 334.03 Developmental Performance Polypropylene Resin is a propylene-based resin intended for use in extrusion blow molded containers requiring improved impact resistance. Targeted end-use app.. |