Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1650 MPa | 239000 psi | ASTM D790A |
SABIC PP 526P Polypropylene Homopolymer for Cast Film Product Description: PP 526P is specially developed for cast film applications for producing clear films and does not contain slip or antiblock additives.Films produced using PP 526P will exhibit:C.. |
|||
Flexural Modulus, 1% Secant | 1650 MPa | 239000 psi | ASTM D790 |
Entec Hypro™ PP-HP10 Homopolymer, 10 Melt Flow This product is intended for general purpose injection molding applications such as caps and closures, resin furniture and consumer products.Information provided by Entec |