Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1080 MPa | 157000 psi | ASTM-D790 |
Braskem GM7040G HDPE High Density Extrusion Polyethylene GM7040G is a high-density polyethylene compound specially developed for the manufacturing of extruded pipes for a gas pressurized line. It is produced with bimodal technology and has high molar mass.. |
|||
Flexural Modulus, 1% Secant | 1080 MPa | 157000 psi | ASTM D790 |
Braskem Green PE SGM7746C Blow Molding and Monofilament High Density Polyethylene Lower greenhouse gas emissions100% made from renewable raw materialsPerformance and Competitiveness: Green Polyethylene has the same characteristics as petrochemical polyethyleneApplications: Mono.. |