Polymer Property : Flexural Modulus, 1% Secant = 1550 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 1550 MPa
225000 psi
ASTM D790A
SABIC PP 413MNK45 Polypropylene Impact Copolymer for Injection Molding
Product Description: PP 413MNK45 is a controlled rheology PP grade with a very high fluidity. It is provided with an antistatic package & nucleating agent and is especially developed for producing..
Flexural Modulus, 1% Secant 1550 MPa
225000 psi
ASTM D790A
SABIC PP 518A Polypropylene Homopolymer for Fiber Applications
Product Description: PP 518A is a PP homopolymer with a broad molecular weight distribution intended for fiber extrusion applications.PP 518A has the following features:Consistent processabilityGoo..
Flexural Modulus, 1% Secant 1550 MPa
225000 psi
ASTM D790A
SABIC PP 518P Polypropylene Homopolymer for Fiber Applications
Product Description: PP 518P is a PP homopolymer with a broad molecular weight distribution intended for fiber extrusion applications.PP 518P has the following features:Consistent processabilityGoo..
Flexural Modulus, 1% Secant 1550 MPa
225000 psi
ASTM D790A
SABIC PP 524P Polypropylene Homopolymer for Bi-axially Oriented Film
Product Description: PP 524P is a non formulated grade, specially developed for bi-axially oriented PP (BOPP) film extrusion with a very specific molecular structure providing ultimate properties r..
Flexural Modulus, 1% Secant 1550 MPa
225000 psi
ASTM D790A
SABIC PP 529P Polypropylene Homopolymer for Bi-axially Oriented Film
Product Description: PP 529P is a non formulated grade, specially developed for bi-axially oriented PP (BOPP) film extrusion with a very specific molecular structure providing ultimate properties r..
Flexural Modulus, 1% Secant 1550 MPa
225000 psi
ASTM D790A
SABIC PP 5701P Polypropylene Homopolymer for Injection Molding
Product Description: PP 5701P is specially for producing rigid injection molded articles for general purpose applications. It gives consistent processability and high gloss in the products.Typical..
Flexural Modulus, 1% Secant 1550 MPa
225000 psi
ASTM D790A
SABIC PP 5702P Polypropylene Homopolymer for Injection Molding
Product Description: PP 5702P is specially developed for rigid injection molded articles for general purpose applications. It gives consistent processability and high gloss in the products.Typical..
Flexural Modulus, 1% Secant 1550 MPa
225000 psi
ASTM D790A
SABIC PP 5703P Polypropylene Homopolymer for Injection Molding
Product Description: PP 5702P is specially developed for producing rigid injection molded articles for general purpose applications. It gives consistent processability and high gloss in the produc..
Flexural Modulus, 1% Secant 1550 MPa
225000 psi
ASTM D790
Entec Hypro™ PP-HP35NS Homopolymer, 35 Melt Flow
This product is intended for thin-wall injection molding applications as well as low denier filament yarns, extrusion coating and specialty cast embossed film.Information provided by Entec