Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1360 MPa | 197000 psi | ASTM D790 |
Dow H349-02 Polypropylene Homopolymer Resin H349-02 Polypropylene Resin intended for use in biaxial oriented (BOPP) film processes. This product can also be used in extrusion and thermoforming applications where improved melt strength is des.. |
|||
Flexural Modulus, 1% Secant | 1360 MPa | 197000 psi | ASTM D790 |
Braskem JV060U Injection Molding High Density Polyethylene Boxes for beverages bottles; Boxes in general; Technical parts.Information provided by Braskem. |