Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1060 MPa | 154000 psi | ASTM D790 |
Flint Hills 23T2A Random Copolymer Polypropylene Features: Clarified, autoclave and good impact strength. Product does not contain animal derived components.Applications: Designed for Blow molding and ThermoformingInformation provided by Flint H.. |
|||
Flexural Modulus, 1% Secant | 1060 MPa | 154000 psi | ASTM D790B |
Teknor Apex Terraloy™ BP 13000A Thermoplastic Starch + PP Notes: Terraloy™ BP-13000A is a Thermoplastic Starch/PP ready-to-process compound that contains up to 30% of TPS renewable content. This compound is intended for injection molding as well as extru.. |