Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1050 MPa | 152000 psi | ASTM D790A |
SABIC PP 674K Polypropylene Copolymer for Injection Molding Product Description: PP 674K is specially developed for producing injection molded & ISBM articles with high clarity and also has better impact properties than homo PP counterparts.PP 674K has the .. |
|||
Flexural Modulus, 1% Secant | 1050 MPa | 152000 psi | ASTM D790A |
SABIC PP681K Polypropylene Random Copolymer for Injection Molding Product Description: PP 681K is specially developed for producing injection molded articles with high clarity and also has better impact properties than homo PP counterparts.PP 681K has the followi.. |
|||
Flexural Modulus, 1% Secant | 1050 MPa | 153000 psi | 0.05 in/min; ASTM D790A |
ExxonMobil PP9074MED Polypropylene Homopolymer Product Description: A highly clarified random copolymer resin designed for injection molding of medical devices suitable for sterilization by high energy radiation.Availability: Europe and North A.. |
|||
Flexural Modulus, 1% Secant | 1050 MPa | 153000 psi | 0.5 in/min; ASTM D790B |
ExxonMobil PP9513 Polypropylene Homopolymer Product Description: A random copolymer resin designed for non-oriented film.Availability: North America Features:Controlled RheologyEthylene Oxide SterilizableUses: BagsCast FilmHeavy-duty BagsPac.. |