Polymer Property : Tear Strength = 64.0 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 64.0 kN/m

@Thickness 2.00 mm,
Temperature 23.0 °C
365 pli

@Thickness 0.0787 in,
Temperature 73.4 °F
Method A, Trouser; Across Flow; ISO 34-1
PolyOne OnFlex™ BIO 5380A-E0006 Thermoplastic Elastomer (TPE)
OnFlex™ BIO 5300 series thermoplastic elastomer compounds are soft thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% of renewable materi..
Tear Strength 64.0 kN/m

@Thickness 2.00 mm,
Temperature 23.0 °C
365 pli

@Thickness 0.0787 in,
Temperature 73.4 °F
Method A, Trouser; Flow; ISO 34-1
PolyOne OnFlex™ BIO 5380A-E0006 Thermoplastic Elastomer (TPE)
OnFlex™ BIO 5300 series thermoplastic elastomer compounds are soft thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% of renewable materi..