Mechanical Properties Metric English Comments
Tensile Strength at Break 30.0 MPa

@Temperature 90.0 °C
4350 psi

@Temperature 194 °F
LATI Kelon® B FR H2 CE/25-V2HF PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Eur..
Tensile Strength at Break 30.0 MPa

@Temperature 150 °C
4350 psi

@Temperature 302 °F
LATI Larpeek 50 PEEK
Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;..
Tensile Strength at Break 30.0 MPa

@Temperature 90.0 °C
4350 psi

@Temperature 194 °F
LATI Lastilac RT K/10 ABS, 10% Carbon Fiber Reinforced
Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. Carbon fiber. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInforma..
Tensile Strength at Break 30.0 MPa

@Temperature 150 °C
4350 psi

@Temperature 302 °F
LATI Latamid 66 E21 G/15 PA 66, 15% Glass Fiber Reinforced
Polyamide 66 (PA66) based compound. Toughened. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici..
Tensile Strength at Break 30.0 MPa

@Temperature 90.0 °C
4350 psi

@Temperature 194 °F
LATI Kelon® B FR H CET/30-V0 PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Low thermal expansion coefficient. Very high dimensional stab..
Tensile Strength at Break 30.0 MPa

@Temperature 90.0 °C
4350 psi

@Temperature 194 °F
LATI Kelon® B H CET/30 PA 6, 30% Mineral Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. Very high dimensional stability. Good elongationAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Amer..
Tensile Strength at Break 30.0 MPa

@Temperature 120 °C
4350 psi

@Temperature 248 °F
LATI Kelon® B H CETG/300 PA 6, Glass/Mineral Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
Tensile Strength at Break 30.0 MPa

@Temperature 150 °C
4350 psi

@Temperature 302 °F
LATI Larton CE/60 PPS, 60% Mineral Reinforced
Polyphenylene Sulfide (PPS) based compound. Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; ..
Tensile Strength at Break 30.0 MPa

@Temperature 120 °C
4350 psi

@Temperature 248 °F
LATI Latamid 6 H2 G/20-V2HF PA 6, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Euro..
Tensile Strength at Break 30.0 MPa

@Temperature 120 °C
4350 psi

@Temperature 248 °F
LATI Latamid 66 S/30 PA 66, 30% Glass Bead Reinforced
Polyamide 66 (PA66) based compound. Glass beads. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Tensile Strength at Break 30.0 MPa

@Temperature 60.0 °C
4350 psi

@Temperature 140 °F
LATI Latan 13 S/15 POM, 15% Glass Bead Reinforced
Polyoxymethylene (POM) based compound. Glass beads. Medium viscosity. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro..
Tensile Strength at Break 30.0 MPa

@Temperature 60.0 °C
4350 psi

@Temperature 140 °F
LATI Latan 13 S/20 POM, 20% Glass Bead Reinforced
Polyoxymethylene (POM) based compound. Glass beads. Medium viscosity. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro..
Tensile Strength at Break 30.0 MPa

@Temperature 90.0 °C
4350 psi

@Temperature 194 °F
LATI Latene® AG3H2W G/30-V0E PP Homopolymer, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Metal stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE freeAvailability: A..
Tensile Strength at Break 30.0 MPa

@Temperature 90.0 °C
4350 psi

@Temperature 194 °F
LATI Later 4 G/30-V0CT2 PBT, 30% Glass Fiber Reinforced, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Tensile Strength at Break 30.0 MPa

@Temperature 60.0 °C
4350 psi

@Temperature 140 °F
LATI Latilon 28D-V0 PC, Flame Retardant
Polycarbonate (PC) based compound. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. Very high dimensional stability. Ve..
Tensile Strength at Break 30.0 MPa

@Temperature 150 °C
4350 psi

@Temperature 302 °F
LATI Kelon® A FR H2 CETG/300-V0 PA 66, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion ..
Tensile Strength at Break 30.0 MPa

@Temperature 150 °C
4350 psi

@Temperature 302 °F
LATI Later 4E61 GCER/450-V0 PBT, Glass/Mineral Filled, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. Toughened. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very good electrical properties.Avail..
Tensile Strength at Break 30.0 MPa

@Temperature 23.0 °C
4350 psi

@Temperature 73.4 °F
LATI Latiblend 7587 E61-V0 PBT/PC, Flame Retardant
Blend based on Polybutylene Terephthalate (PBT) / Polycarbonate (PC). Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very high dimensional stability. High impact re..
Tensile Strength at Break 30.0 MPa

@Temperature 275 °C
4350 psi

@Temperature 527 °F
ISO 527
Victrex® PEEK 650GL30 30% Glass Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, color natural/beige.Typical..