Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 18.7 MPa @Temperature 100 °C, Time 259000 sec |
2710 psi @Temperature 212 °F, Time 72.0 hour |
Circulating Oven Aging |
LG Chemical NBR 7150 High Acrylonitrile Polymer Description: NBR 7150 is a copolymer of butadiene and acrylonitrile manufactured by cold emulsion polymerization technology of Goodyear Tire and Rubber Company, USA. NBR 7150 is a non staining, medi.. |