Polymer Property : Tensile Strength at Break = 23200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 160 MPa

@Temperature 23.0 °C
23200 psi

@Temperature 73.4 °F
ISO 527-2
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi..
Tensile Strength at Break 160 MPa

@Temperature 23.0 °C
23200 psi

@Temperature 73.4 °F
ISO 527
Victrex® PEEK 150GL20 Polyetheretherketone, 20% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 20% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta..
Tensile Strength at Break 160 MPa

@Temperature 125 °C
23200 psi

@Temperature 257 °F
ISO 527
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced
General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex.
Tensile Strength at Break 160 MPa

@Temperature -50.0 °C
23200 psi

@Temperature -58.0 °F
ASTM D638
Gharda Chemicals G-PAEKâ„¢ 1230FC Ultra High Performance PEK Polymer
Product Details: Ultra High Performance Thermoplastic material, 10% carbon fiber, 10% PTFE and 10% graphite reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection mo..
Tensile Strength at Break 160 MPa

@Temperature 23.0 °C
23200 psi

@Temperature 73.4 °F
LATI Larpeek 10 GCE/600 PEEK, Glass/Mineral Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa ..
Tensile Strength at Break 160 MPa

@Temperature 60.0 °C
23200 psi

@Temperature 140 °F
LATI Larpeek 50 G/30 PEEK, 30% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Strength at Break 160 MPa

@Temperature 60.0 °C
23200 psi

@Temperature 140 °F
LATI Larton K/40 HM PPS, 40% Carbon Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af..
Tensile Strength at Break 160 MPa

@Temperature 23.0 °C
23200 psi

@Temperature 73.4 °F
LATI Larton L G/40 L-PPS, 40% Glass Fiber Reinforced
Linear Polyphenylene Sulfide (L-PPS) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle..
Tensile Strength at Break 160 MPa

@Temperature 23.0 °C
23200 psi

@Temperature 73.4 °F
LATI Latamid 6 H2 G/30 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla..
Tensile Strength at Break 160 MPa

@Temperature 60.0 °C
23200 psi

@Temperature 140 °F
LATI Latamid 66 H2 K/30 PA 66, 30% Carbon Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl..
Tensile Strength at Break 160 MPa

@Temperature 150 °C
23200 psi

@Temperature 302 °F
LATI Larpeek 10 G/60 PEEK, 60% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Strength at Break 160 MPa

@Temperature 150 °C
23200 psi

@Temperature 302 °F
LATI Larpeek 10 K/20 PEEK, 20% Carbon Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Strength at Break 160 MPa

@Temperature 60.0 °C
23200 psi

@Temperature 140 °F
LATI Latamid 6 H2 G/50 PA 6, 50% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla..
Tensile Strength at Break 160 MPa

@Temperature 23.0 °C
23200 psi

@Temperature 73.4 °F
LATI Latamid 66 H2 G/25 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop..
Tensile Strength at Break 160 MPa

@Temperature 23.0 °C
23200 psi

@Temperature 73.4 °F
2; ISO 527-2
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA), 16% Glass Fiber (Dry)
Amodel® AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s..
Tensile Strength at Break 160 MPa

@Temperature 23.0 °C
23200 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® RS 30G30L NC010 Nylon 610  (Unverified Data**)
Zytel® RS 30G30L NC010 is a lubricated, 30% glass fiber reinforced polyamide 610 resin containing a minimum of 40% renewably sourced ingredients by weight (60% based on polymer only). It was initia..
Tensile Strength at Break 160 MPa

@Temperature 23.0 °C
23200 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 70G43HSLA BK099 Nylon 66  (Unverified Data**)
Zytel® 70G43HSLA BK099 is a 43% glass fiber reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Strength at Break 160 MPa

@Temperature -40.0 °C
23200 psi

@Temperature -40.0 °F
ISO 527
DuPont Performance Polymers Rynite® 940 BK505 PET  (Unverified Data**)
Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers
Tensile Strength at Break 160 MPa

@Temperature 23.0 °C
23200 psi

@Temperature 73.4 °F
ISO 527
Victrex® PEEK 150FC30 Easy Flow
Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy ..