Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 211 MPa @Temperature 23.0 °C |
30600 psi @Temperature 73.4 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Typical applications include .. |
|||
Tensile Strength at Break | 211 MPa @Temperature 23.0 °C |
30600 psi @Temperature 73.4 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Dry) Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre.. |
|||
Tensile Strength at Break | 211 MPa @Temperature 23.0 °C |
30600 psi @Temperature 73.4 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Testing conducted on samp.. |
|||
Tensile Strength at Break | 211 MPa @Temperature 23.0 °C |
30600 psi @Temperature 73.4 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)
(Unverified Data**) Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength.. |
|||
Tensile Strength at Break | 211 MPa @Temperature 23.0 °C |
30600 psi @Temperature 73.4 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp.. |