Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 200 MPa @Temperature 23.0 °C |
29000 psi @Temperature 73.4 °F |
ISO 527 |
Victrex® PEEK 150GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact c.. |
|||
Tensile Strength at Break | 200 MPa @Temperature 23.0 °C |
29000 psi @Temperature 73.4 °F |
ISO 527 |
Victrex® PEEK -HT™ 22GL30 Polyetherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact comp.. |
|||
Tensile Strength at Break | 200 MPa @Temperature 23.0 °C |
29000 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 70G35HSL BK039B Nylon 66
(Unverified Data**) Zytel® 70G35HSL BK039B is a 35% glass fiber reinforced, heat stabilized, black polyamide 66 for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Strength at Break | 200 MPa @Temperature 150 °C |
29000 psi @Temperature 302 °F |
|
LATI Larpeek 10 K/40 PEEK, 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Strength at Break | 200 MPa @Temperature 60.0 °C |
29000 psi @Temperature 140 °F |
|
LATI Larpeek 50 K/30 PEEK, 30% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Strength at Break | 200 MPa @Temperature 23.0 °C |
29000 psi @Temperature 73.4 °F |
|
LATI Laramid G/30 PPA, 30% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Tensile Strength at Break | 200 MPa @Temperature 90.0 °C |
29000 psi @Temperature 194 °F |
|
LATI Larpeek 10 G/60 PEEK, 60% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Strength at Break | 200 MPa @Temperature 23.0 °C |
29000 psi @Temperature 73.4 °F |
|
LATI Latamid 6 H2 G/65 PA 6, 65% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla.. |
|||
Tensile Strength at Break | 200 MPa @Temperature 23.0 °C |
29000 psi @Temperature 73.4 °F |
|
LATI Latigloss 62 H2 G/50 PA 6, 50% Glass Fiber Reinforced, Heat Stabilized Product with high mechanical properties and exceptional surface finish based on Polyamide 6 (PA6). Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Ameri.. |
|||
Tensile Strength at Break | 200 MPa @Temperature 23.0 °C |
29000 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® HTN 52G35HSL NC010 Polyphthalamide (PPA) Zytel® HTN52G35HSL NC010 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds.Information provided by DuPont Performance .. |
|||
Tensile Strength at Break | 200 MPa @Temperature 23.0 °C |
29000 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612
(Unverified Data**) Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Strength at Break | 200 MPa @Temperature 23.0 °C |
29000 psi @Temperature 73.4 °F |
|
LATI Latamid 66 H2 K/20 PA 66, 20% Carbon Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |