Polymer Property : Tensile Strength at Break = 20.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 20.0 MPa

@Thickness 2.00 mm,
Temperature 23.0 °C
2900 psi

@Thickness 0.0787 in,
Temperature 73.4 °F
Type 1, 200 mm/min Across Flow; DIN 53504
PolyOne OnFlex™ BIO 5380A-E0006 Thermoplastic Elastomer (TPE)
OnFlex™ BIO 5300 series thermoplastic elastomer compounds are soft thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% of renewable materi..
Tensile Strength at Break 20.0 MPa

@Temperature 23.0 °C
2900 psi

@Temperature 73.4 °F
ASTM D638
DuPont Performance Polymers Hytrel® 4069 TPC-ET  (Unverified Data**)
Hytrel® 4069 is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injection..
Tensile Strength at Break 20.0 MPa

@Temperature 120 °C
2900 psi

@Temperature 248 °F
LATI Kelon® B FR H2 CE/25-V2HF PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Eur..
Tensile Strength at Break 20.0 MPa

@Temperature 150 °C
2900 psi

@Temperature 302 °F
LATI Kelon® B H CER/30 PA 6, 30% Mineral Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. Very high dimensional stability. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ame..
Tensile Strength at Break 20.0 MPa

@Temperature 120 °C
2900 psi

@Temperature 248 °F
LATI Laril 13-V1KC PPOm, Mineral Reinforced, Flame Retardant
Modified Polyphenylene Oxide (PPOm) based compound. Mineral filler. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. High dimensional stability. Good therm..
Tensile Strength at Break 20.0 MPa

@Temperature 90.0 °C
2900 psi

@Temperature 194 °F
LATI Lastilac 10 ABS/PC
ABS/PC Blend (ABS/PC). Unfilled. Very good surface appearance. High impact resistance. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaI..
Tensile Strength at Break 20.0 MPa

@Temperature 120 °C
2900 psi

@Temperature 248 °F
LATI Latamid 6 H2 G/20-V0 PA 6, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia ..
Tensile Strength at Break 20.0 MPa

@Temperature 150 °C
2900 psi

@Temperature 302 °F
LATI Kelon® B FR H CET/30-V0 PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Low thermal expansion coefficient. Very high dimensional stab..
Tensile Strength at Break 20.0 MPa

@Temperature 150 °C
2900 psi

@Temperature 302 °F
LATI Kelon® B H CET/30 PA 6, 30% Mineral Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. Very high dimensional stability. Good elongationAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Amer..
Tensile Strength at Break 20.0 MPa

@Temperature 120 °C
2900 psi

@Temperature 248 °F
LATI Laril 13 G/20-V1 PPOm, 20% Glass Fiber Reinforced, Flame Retardant
Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. High dimensional stability. Good thermal..
Tensile Strength at Break 20.0 MPa

@Temperature 150 °C
2900 psi

@Temperature 302 °F
LATI Latamid 6 H2 G/30-V2HF PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-2 classified, halogens-based flame retardants and red phosphorous freeAvailability: Africa & Middle East; Asia Pacific; Europe..
Tensile Strength at Break 20.0 MPa

@Temperature 150 °C
2900 psi

@Temperature 302 °F
LATI Latamid 6 S/30 PA 6, 30% Glass Bead Reinforced
Polyamide 6 (PA6) based compound. Glass beads. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu..
Tensile Strength at Break 20.0 MPa

@Temperature 120 °C
2900 psi

@Temperature 248 °F
LATI Later 4 G/30-V0CT2 PBT, 30% Glass Fiber Reinforced, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Tensile Strength at Break 20.0 MPa

@Temperature 23.0 °C
2900 psi

@Temperature 73.4 °F
LATI Latene® 9H TES/30 PP Homopolymer, Heat Stabilized
Polypropylene homopolymer (PPh) based compound. Heat stabilized. Aesthetic talc.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind..
Tensile Strength at Break 20.0 MPa

@Temperature 90.0 °C
2900 psi

@Temperature 194 °F
LATI Later 4-V0 PBT, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide freeAvailability: Africa & Middle East; Asia Pacific; Europe; L..
Tensile Strength at Break 20.0 MPa

@Temperature 60.0 °C
2900 psi

@Temperature 140 °F
LATI Latiblend 7587 E61-V0 PBT/PC, Flame Retardant
Blend based on Polybutylene Terephthalate (PBT) / Polycarbonate (PC). Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very high dimensional stability. High impact re..
Tensile Strength at Break 20.0 MPa

@Temperature 150 °C
2900 psi

@Temperature 302 °F
LATI Kelon® A FR H2 CET/35-V2 PA 66, 35% Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Mineral filler. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Europe; La..
Copyright © lookpolymers.com All Rights Reserved