Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 188 MPa @Temperature 23.0 °C |
27300 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66
(Unverified Data**) Zytel® 70G25HSL NC010 is a 25% glass fiber reinforced, heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |