Polymer Property : Tensile Strength at Break = 180 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 180 MPa

@Temperature 150 °C
>= 26100 psi

@Temperature 302 °F
PEAK Werkstoff DISPAL S225 Aluminum Alloy, AlSi35Fe2Ni, Condition F
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
Tensile Strength at Break 180 MPa

@Temperature 23.0 °C
26100 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® HTN FG52G35HSL BK011 Polyphthalamide (PPA)  (Unverified Data**)
Zytel®® HTNFG52G35HSL BK011 is a 35% glass reinforced, lubricated, heat stabilized high performance polyamide resin, developed for consideration into applications for the food industry. It is also..
Tensile Strength at Break 180 MPa

@Temperature 23.0 °C
26100 psi

@Temperature 73.4 °F
ISO 527
Victrex® PEEK 150FW30 PEEK, 30% Carbon Fibre/PTFE Reinforced
Product Description:High performance thermoplastic material, 30% reinforced with carbon fibre / PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA fo..
Tensile Strength at Break 180 MPa

@Temperature 125 °C
26100 psi

@Temperature 257 °F
ISO 527
Victrex® PEEK 90CA30 Polyetheretherketone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food cont..
Tensile Strength at Break 180 MPa

@Temperature 23.0 °C
26100 psi

@Temperature 73.4 °F
ISO 527
Victrex® PEEK 90GL30 BLACK EU 30% Glass Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, FDA and EU food contact compliant, ..
Tensile Strength at Break 180 MPa

@Temperature 125 °C
26100 psi

@Temperature 257 °F
ISO 527
Victrex® ST™ ST45CA30 PolyEtherKetoneEtherKetoneKetone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, ..
Tensile Strength at Break 180 MPa

@Temperature 23.0 °C
26100 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 70G25HSLR NC010 Nylon 66  (Unverified Data**)
Zytel® 70G25HSLR NC010 is a 25% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Strength at Break 180 MPa

@Temperature 23.0 °C
26100 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 73G30HSL BK261 Nylon 6  (Unverified Data**)
Zytel® 73G30HSL BK261 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 for injection molding. It has excellent surface appearance and gloss.Information provided by Du..
Tensile Strength at Break 180 MPa

@Temperature 60.0 °C
26100 psi

@Temperature 140 °F
LATI Laramid G/35 PPA, 35% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Tensile Strength at Break 180 MPa

@Temperature 90.0 °C
26100 psi

@Temperature 194 °F
LATI Larpeek 50 K/30 PEEK, 30% Carbon Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Strength at Break 180 MPa

@Temperature 23.0 °C
26100 psi

@Temperature 73.4 °F
LATI Latamid 66 E21 K/30 PA 66, 30% Carbon Fiber Reinforced
Polyamide 66 (PA66) based compound. Toughened. Carbon fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastic..
Tensile Strength at Break 180 MPa

@Temperature 23.0 °C
26100 psi

@Temperature 73.4 °F
LATI Latamid 66 H2 G/50-V0KB1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInf..
Tensile Strength at Break 180 MPa

@Temperature 23.0 °C
26100 psi

@Temperature 73.4 °F
LATI Latamid 66 LH2 G/35 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Oil stabilized. Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
Tensile Strength at Break 180 MPa

@Temperature 120 °C
26100 psi

@Temperature 248 °F
LATI Larpeek 10 G/60 PEEK, 60% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Strength at Break 180 MPa

@Temperature 60.0 °C
26100 psi

@Temperature 140 °F
LATI Larton G/40 I6 PPS, 40% Glass Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Glass fibers. Good elongation. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa ..
Tensile Strength at Break 180 MPa

@Temperature 60.0 °C
26100 psi

@Temperature 140 °F
LATI Latigloss 66 H2 G/60 PA 66, 60% Glass Fiber Reinforced, Heat Stabilized
Product with high mechanical properties and exceptional surface finish based on Polyamide 66 (PA66). Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am..
Tensile Strength at Break 180 MPa

@Temperature 23.0 °C
26100 psi

@Temperature 73.4 °F
LATI Latiohm 66-06 PD03 G/20 PA66, 20% Glass Fiber Reinforced
Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind..
Tensile Strength at Break 180 MPa

@Temperature 1093 °C
26100 psi

@Temperature 1999 °F
Plate; Longitudinal
Special Metals INCONEL® alloy MA758 Ni-Cr Superalloy
INCONEL® alloy MA 758 is an oxide-dispersion-strengthened (ODS) nickel-chromium superalloy, made by mechanical alloying. It is a development of the well-established aerospace superalloy, INCONEL..
Tensile Strength at Break 180 MPa

@Temperature 23.0 °C
26100 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® HTN 52G35HSL NC010 Polyphthalamide (PPA)
Zytel® HTN52G35HSL NC010 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds.Information provided by DuPont Performance ..