Polymer Property : Tensile Strength at Break = 135 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 135 MPa

@Temperature 90.0 °C
19600 psi

@Temperature 194 °F
LATI Larpeek 10 GCE/600 PEEK, Glass/Mineral Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa ..
Tensile Strength at Break 135 MPa

@Temperature 120 °C
19600 psi

@Temperature 248 °F
LATI Larpeek 50 G/30 PEEK, 30% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Strength at Break 135 MPa

@Temperature 60.0 °C
19600 psi

@Temperature 140 °F
LATI Larton K/20 PPS, 20% Carbon Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Strength at Break 135 MPa

@Temperature 90.0 °C
19600 psi

@Temperature 194 °F
LATI Latamid 6 H2 G/55 PA 6, 55% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla..
Tensile Strength at Break 135 MPa

@Temperature 90.0 °C
19600 psi

@Temperature 194 °F
LATI Latamid 66 H2 K/30 PA 66, 30% Carbon Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl..
Tensile Strength at Break 135 MPa

@Temperature 23.0 °C
19600 psi

@Temperature 73.4 °F
LATI Larpeek 10 G/15 PEEK, 15% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Strength at Break 135 MPa

@Temperature 120 °C
19600 psi

@Temperature 248 °F
LATI Larpeek 10 G/30 PEEK, 30% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Strength at Break 135 MPa

@Temperature 23.0 °C
19600 psi

@Temperature 73.4 °F
LATI Latamid 66 H2 G/25-V0CT1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Lat..
Tensile Strength at Break 135 MPa

@Temperature 60.0 °C
19600 psi

@Temperature 140 °F
LATI Latamid 66 H2 G/30 PA 66, 30% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop..
Tensile Strength at Break 135 MPa

@Temperature 23.0 °C
19600 psi

@Temperature 73.4 °F
LATI Later 4 G/50 PBT, 50% Glass Fiber Reinforced
Polybutylene Terephthalate (PBT) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast..
Tensile Strength at Break 135 MPa

@Temperature 23.0 °C
19600 psi

@Temperature 73.4 °F
LATI Latilon 28D K/40 PC, 40% Carbon Fiber Reinforced
Polycarbonate (PC) based compound. Carbon fiber. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided b..
Tensile Strength at Break 135 MPa

@Temperature 60.0 °C
19600 psi

@Temperature 140 °F
LATI Latiohm 66-06 PD03 G/20 PA66, 20% Glass Fiber Reinforced
Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind..
Tensile Strength at Break 135 MPa

@Temperature 23.0 °C
19600 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® HTN FR52G20NH BK337 Polyphthalamide (PPA)
Zytel® HTNFR52G20NH BK337 is a 20% glass reinforced, flame retardant, lubricated high performance polyamide resin. It is also a PPA resin and it uses a non-halogenated flame retardant.Information p..
Tensile Strength at Break 135 MPa

@Temperature 23.0 °C
19600 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® PLUS PLS95G35DH1 BK031 Nylon
Zytel® PLS95G35DH1 BK031is a high flow 35% glass reinforced PA using SHIELD Technology, only from DuPont, combining excellent surface appearance, excellent welding and fatigue retention, exceptiona..
Tensile Strength at Break 135 MPa

@Temperature 100 °C
19600 psi

@Temperature 212 °F
ASTM D638
Gharda Chemicals G-PAEK™ 1230GF Ultra High Performance PEK Polymer
Product Details: Ultra High Performance Thermoplastic material, 30% glass fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, standard flow, Beige ..
Tensile Strength at Break 135 MPa

@Temperature 23.0 °C
19600 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTNFR52G30NHF BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin with improved flow. It is also a PPA resin and it uses a non-halogenated flame ret..
Tensile Strength at Break 135 MPa

@Temperature 23.0 °C
19600 psi

@Temperature 73.4 °F
LATI Latamid 66 H2 G/25-V0KB3 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..