Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Thickness 4.00 mm,
Temperature 23.0 °C
38.1 ft-lb/in²

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Premix Thermoplastics PRE-ELEC® PE 1297 Conductive Thermoplastic Compound
PRE-ELEC® PE 1297 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PE..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
d.a.m.; ISO 180-1A
Lanxess Durethan® DP 2325 H3.0 DUS031 000000 Nylon 66
PA 66, non-reinforced, injection molding, improved flowability, impact modified, heat-aging stabilizedInformation provided by LANXESS.
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Styrolution Terblend® N NM-21 EF Gray 38058 ABS+PA (Conditioned)
Description: Terblend® N NM-21 EF is an UV stabilized ABS/PA blend combining very high impact strength, even at low temperatures. The enhanced flowability enables excellent processability and sur..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP Thermocomp R1000HI620 PA 66 (Europe-Africa-Middle East)
Impact modified Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched (ISO) >= 80.0 kJ/m²

@Temperature 23.0 °C
>= 38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Total PPC 1640 Polypropylene, Heterophasic Copolymer, Non-pressure Pipes
Polypropylene PPC 1640 is a nucleated heterophasic (block) copolymer with a Melt Flow index of 0.3 g/10 min. This resin has a long-term heat stabilization package. It exhibits high stiffness in co..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Thickness 3.20 mm,
Temperature 23.0 °C
38.1 ft-lb/in²

@Thickness 0.126 in,
Temperature 73.4 °F
partial break; b.o. ISO 180-A
Covestro Makrolon® 1952 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Me..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Thickness 3.20 mm,
Temperature 23.0 °C
38.1 ft-lb/in²

@Thickness 0.126 in,
Temperature 73.4 °F
partial break; b.o. ISO 180-A
Covestro Makrolon® 2600 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Thickness 3.20 mm,
Temperature 23.0 °C
38.1 ft-lb/in²

@Thickness 0.126 in,
Temperature 73.4 °F
partial break; b.o. ISO 180-A
Covestro Makrolon® 2652 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Thickness 3.20 mm,
Temperature 23.0 °C
38.1 ft-lb/in²

@Thickness 0.126 in,
Temperature 73.4 °F
partial break; b.o. ISO 180-A
Covestro Makrolon® 2665 MAS071 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Thickness 3.20 mm,
Temperature 23.0 °C
38.1 ft-lb/in²

@Thickness 0.126 in,
Temperature 73.4 °F
partial break; b.o. ISO 180-A
Covestro Makrolon® 2665 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medium viscosity, easy..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Thickness 3.20 mm,
Temperature 23.0 °C
38.1 ft-lb/in²

@Thickness 0.126 in,
Temperature 73.4 °F
partial break; b.o. ISO 180-A
Covestro Makrolon® 2667 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
Edgew 80x10x4 sp=62; ISO 180/1A
Eurostar Staramide AST44 PA66, Impact Modified, Injection Molded
AST44 is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Eurotec® Tecomid® NB40 NL IH PA 6 impact modified
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Thickness 3.20 mm,
Temperature 23.0 °C
38.1 ft-lb/in²

@Thickness 0.126 in,
Temperature 73.4 °F
partial break; b.o. ISO 180-A
Covestro Makrolon® ET2613 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• Medium vi..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Thickness 3.20 mm,
Temperature 23.0 °C
38.1 ft-lb/in²

@Thickness 0.126 in,
Temperature 73.4 °F
partial break; b.o. ISO 180-A
Covestro Makrolon® ET3127 Polycarbonate
Makrolon® polycarbonate resinMain characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characterist..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Thickness 3.20 mm,
Temperature 23.0 °C
38.1 ft-lb/in²

@Thickness 0.126 in,
Temperature 73.4 °F
partial break; b.o. ISO 180-A
Covestro Makrolon® ET3227 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
80x10x4; ISO 180/1A
Eurostar Staramide R1000HI620 PA66, Impact Modified, Injection Molded
Staramide R1000HI620 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI010)Information provided by Eurostar.
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Thickness 3.20 mm,
Temperature 23.0 °C
38.1 ft-lb/in²

@Thickness 0.126 in,
Temperature 73.4 °F
partial break; b.o. ISO 180-A
Covestro Makrolon® LED2643 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• LED lighting, optics, ..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Thickness 3.20 mm,
Temperature 23.0 °C
38.1 ft-lb/in²

@Thickness 0.126 in,
Temperature 73.4 °F
partial break; b.o. ISO 180-A
Covestro Makrolon® LQ2647 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Optical lens, safety g..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
partial break; 50%RH; ISO 180/1A
DuPont Performance Polymers Zytel® RS 3261THSL BK041A Nylon 610  (Unverified Data**)
Zytel® RS 3261THSL BK041A is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by weight. It is a black, unreinforced, toughened and heat stabilised r..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
partial break; 50%RH; ISO 180/1A
DuPont Performance Polymers Zytel® RS 3261TL NC010 Nylon 610  (Unverified Data**)
Zytel® RS 3261TL NC010 is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by weight. It is an unreinforced and toughened resin for injection molding..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180/4A
Mitsubishi Xantar® C CE 407 Polycarbonate/ABS Blend
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher..
Copyright © lookpolymers.com All Rights Reserved