Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Asia Pacific) PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Europe-Africa-Middle East) PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East re.. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 123X PC Copolymer (Europe-Africa-Middle East) Improved flow PC with excellent processability and mold release.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1413T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1413T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 °C) ductility in combination with medium f.. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXD103 PC FXD103 is a Light Diffusion effect, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace.This data was supplied by SABIC-IP for the .. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXD1433T PC Copolymer (Asia Pacific) Clear PC-siloxane copolymer with excellent processability in special light diffusion colors. Medium flow, UV stabilized. Improved toughness compared to standard PC in same color. Color package may .. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXE123R PC (Europe-Africa-Middle East) LEXAN FXE123R is a transparent/translucent, UV stabilised low viscosity grade for special effects colors with a fluorescent appearance. Color package may affect performance.This data was supplied by.. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXE921A PC (Europe-Africa-Middle East) LEXAN FXE921A is a transparent/translucent, medium viscosity, flame retardant grade with a fluorescent appearance. Color package may affect performance.This data was supplied by SABIC-IP for the Eur.. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPX4 PC Copolymer (Europe-Africa-Middle East) Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP.. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® LR180 PC (Europe-Africa-Middle East) LR180 is a medium viscosity, non UV, non release containing multipurpose polycarbonate recycle gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® LR180R PC (Europe-Africa-Middle East) LR180R is a medium viscosity,release containing multipurpose polycarbonate industrial gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Nilit Nilamid A3 H ZC High Impact PA66 Description: Nilamid A3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, .. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXD1413T PC Copolymer (Europe-Africa-Middle East) Clear PC-siloxane copolymer with excellent processability, in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may af.. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXE1413T PC Copolymer Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in "Energy" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color packa.. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXE1413T PC Copolymer (Asia Pacific) Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in "Energy" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color packa.. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXE1414T PC Copolymer (Europe-Africa-Middle East) Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in "Energy" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color packa.. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® SLX1431T PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180/4A |
Mitsubishi Xantar® C CM 406 U Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics PC2200 PC (Asia Pacific) PC2200 resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics PC2200R PC (Asia Pacific) PC2200R resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplied by S.. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics PC2200R PC (Europe-Africa-Middle East) PC2200R resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplied by S.. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics PC2203R PC PC2203R resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli.. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® CL500U PBT+PC (Europe-Africa-Middle East) XENOY CL500U is a semi-crystalline blend, developed for exterior automotive parts ( except bumper shells ) and non automotive parts, requiring good impact, excellent chemical resistance and UV stabi.. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Styrolution Terblend® S NM-31 ASA / PA Terblend® S is a UV-stabilized ASA/PA blend with high impact strength, easy flow and pronounced color fastness. It is especially suitable for unpainted highly UV-exposed automotive interior parts.. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Thickness 3.20 mm, Temperature 23.0 °C |
30.9 ft-lb/in² @Thickness 0.126 in, Temperature 73.4 °F |
partial break; b.o. ISO 180-A |
Covestro Makrolon® Rx1851 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices• Low.. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
partial break; DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® RS 3261THSL BK041A Nylon 610
(Unverified Data**) Zytel® RS 3261THSL BK041A is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by weight. It is a black, unreinforced, toughened and heat stabilised r.. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® ML6240 PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle Eas.. |