Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 6.50 kJ/m² @Thickness 4.00 mm, Temperature -30.0 °C |
3.09 ft-lb/in² @Thickness 0.157 in, Temperature -22.0 °F |
ISO 180/1A |
Polimeri Europa Edistir R 850E Polystyrene Super high impact polystyrene with good heat resistance. Designed for sheet extrusion and thermoforming of deep drawn containers even
diluted with high percentage of GP. Suitable for general injecti.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² @Thickness 4.00 mm, Temperature -30.0 °C |
3.09 ft-lb/in² @Thickness 0.157 in, Temperature -22.0 °F |
ISO 180/1A |
Polimeri Europa Edistir SR 550 Polystyrene High impact, easy flow polystyrene with good elasticity at low temperatures.Suitable for injection moulding of large or complex parts with low thickness and high impact strength.
Designation: Thermo.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Nilit Nilamid A G5 FR C4 25% Glass Fiber Reinforced, Flame Retardant PA66 (with Halogens) Description: Nilamid A G5 FR C4 combines excellent mechanical performance with flame retardancy. The halogenated flame retardant system used in this product allows a wide range of colors. This produ.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² @Temperature -30.0 °C |
3.09 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Nilit Nilamid B G6 FR C4 30% Glass Fiber Reinforced, Flame Retardant PA6 Description: Nilamid B G6 FR C4 combines excellent mechanical performance with flame retardancy. The halogenated flame retardant system used in this product allows a wide range of colors. This produ.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² @Temperature -30.0 °C |
3.09 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Sax Polymers SAXAMID 226F4RY01 Nylon 6.6, 20% Glass Fiber SAXAMID 226F4RY01 is a polyamide 6.6 injection-molding-grade reinforced with 20% glass fibers. It has a halogen-free flame retardant.Information provided by SAX Polymers |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² @Temperature 2.00 °C |
3.09 ft-lb/in² @Temperature 35.6 °F |
ISO 180 |
Total PPC 12642 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 12642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 70 g/10 min and good mechanical properties.Polypropylene PPC 10641 has been developed for high s.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² @Temperature -20.0 °C |
3.09 ft-lb/in² @Temperature -4.00 °F |
ISO 180 |
Total PPC 9612 Polypropylene, Heterophasic Copolymer, Injection Molding This product is a Total Ecosolutions grade.Polypropylene PPC 9612 has been developed specifically for the injection molding of crates and is characterized by a high Melt Flow index of 20 g/10 min. .. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² @Temperature -20.0 °C |
3.09 ft-lb/in² @Temperature -4.00 °F |
ISO 180 |
Total PPC 11812 S01 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 11812 S01 has been developed for high speed injection molding of thin walled packaging containers requiring top level impact resistance at cold temperature (-20°C). It is charact.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² @Temperature -20.0 °C |
3.09 ft-lb/in² @Temperature -4.00 °F |
ISO 180 |
Total PPC 3650 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 3650 is a heterophasic copolymer with a Melt Flow index of 2 g/10 min.Polypropylene PPC 3650 provides an excellent balance between toughness and flow, being particularly suitable i.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultraform® N2320 0035 LEV POM Description: Is a POM, rapidly solidifying standard grade with improved impact strength for injection moldingInformation provided by BASF |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultraform® N2320 006 POM Description: Is a POM, high-molecular-weight grade with somewhat increased flowability for injection molding of relatively thick-walled moldings.Information provided by BASF |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultraform® S2320 0035 POM Description: Is a POM, free-flowing and rapidly solidifying standard grade with improved impact strength for injection molding.Information provided by BASF |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultrason® E 2010 MR SW 10111 PESU Description: Unreinforced, medium viscosity standard injection molding grade, demolding optimized. Abbreviated designation according to ISO 1043-1: PESU.Information provided by BASF |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultrason® E 2010 HC PESU Information provided by BASF |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66
(Unverified Data**) Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² @Temperature -20.0 °C |
3.09 ft-lb/in² @Temperature -4.00 °F |
ISO 180/1A |
Borealis Daplen™ EF103AE Polypropylene TPO Compound Daplen™ EF103AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, high melt flow rate an.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² @Temperature -30.0 °C |
3.09 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R860 BK02 Nylon 66, Glass/Mineral Reinforced, Conditioned Vydyne® R860 BK02 is general-purpose, glass-fiber and mineral-reinforced PA66 resin. Available in black, this product is also lubricated for improved flow and offers superior surface appearance. Gl.. |