Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 4.80 kJ/m² @Temperature -40.0 °C |
2.28 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
Eastman DuraStar DS1000 Polymer, Natural Durastar DS1000 polymer has excellent appearance and clarity. Its most outstanding features are chemical resistance and excellent processing characteristics. Exposure to aromatic oils often causes c.. |
|||
Izod Impact, Notched (ISO) | 4.80 kJ/m² @Temperature -40.0 °C |
2.28 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
Eastman DuraStar DS1110UVI Polymer, Natural Durastar DS1110UVI polymer, contains an ultraviolet light stabilization package. It is recommended for indoor applications requiring enhanced color stability upon extended exposure to fluorescent li.. |
|||
Izod Impact, Notched (ISO) | 4.80 kJ/m² @Temperature -40.0 °C |
2.28 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
Eastman DuraStar MN610 Polymer, Natural Durastar MN610 polymer has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. MN610 has very .. |
|||
Izod Impact, Notched (ISO) | 4.80 kJ/m² @Temperature -40.0 °C |
2.28 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
Eastman DuraStar MN611 Polymer, Natural Durastar Polymer MN611 contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing char.. |