Polymer Property : Izod Impact, Notched (ISO) = 4.30 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 9.03 kJ/m²

@Temperature -30.0 °C
4.30 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Polymer Resources ABS-GP-IM General Purpose ABS, Impact Modified
General Purpose Acrylonitrile Butadiene Styrene, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples...