Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 75.0 kJ/m² @Thickness 4.00 mm, Temperature -20.0 °C |
35.7 ft-lb/in² @Thickness 0.157 in, Temperature -4.00 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PE 1297 Conductive Thermoplastic Compound PRE-ELEC® PE 1297 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PE.. |
|||
Izod Impact, Notched (ISO) | 75.0 kJ/m² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® ML3021A PC (Europe-Africa-Middle East) LEXAN ML3021A is a high viscosity, UV stabilised grade especially designed for injection blow moulding and profile extrusion.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regi.. |
|||
Izod Impact, Notched (ISO) | 75.0 kJ/m² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1A |
Lanxess Durethan® BC 550 DUSXBL 900116 Nylon 6 PA 6, non-reinforced, extrusion, Blastorm, impact modified, heat-ageing stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 75.0 kJ/m² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 180-1A |
Lanxess Durethan® TP 142-011 900116 Nylon 6 PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 75.0 kJ/m² @Thickness 3.20 mm, Temperature 23.0 °C |
35.7 ft-lb/in² @Thickness 0.126 in, Temperature 73.4 °F |
partial break; b.o. ISO 180-A |
Covestro Makrolon® 2400 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Izod Impact, Notched (ISO) | 75.0 kJ/m² @Thickness 3.20 mm, Temperature 23.0 °C |
35.7 ft-lb/in² @Thickness 0.126 in, Temperature 73.4 °F |
partial break; b.o. ISO 180-A |
Covestro Makrolon® 2405 MAS048 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Izod Impact, Notched (ISO) | 75.0 kJ/m² @Thickness 3.20 mm, Temperature 23.0 °C |
35.7 ft-lb/in² @Thickness 0.126 in, Temperature 73.4 °F |
partial break; b.o. ISO 180-A |
Covestro Makrolon® 2407 MAS070 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Izod Impact, Notched (ISO) | 75.0 kJ/m² @Thickness 3.20 mm, Temperature 23.0 °C |
35.7 ft-lb/in² @Thickness 0.126 in, Temperature 73.4 °F |
partial break; b.o. ISO 180-A |
Covestro Makrolon® 2407 MAS145 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Izod Impact, Notched (ISO) | 75.0 kJ/m² @Thickness 3.20 mm, Temperature 23.0 °C |
35.7 ft-lb/in² @Thickness 0.126 in, Temperature 73.4 °F |
partial break; b.o. ISO 180-A |
Covestro Makrolon® 2408 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Izod Impact, Notched (ISO) | 75.0 kJ/m² @Thickness 3.20 mm, Temperature 23.0 °C |
35.7 ft-lb/in² @Thickness 0.126 in, Temperature 73.4 °F |
partial break; b.o. ISO 180-A |
Covestro Makrolon® Rx2435 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices• Low.. |
|||
Izod Impact, Notched (ISO) | 75.0 kJ/m² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
Edgew 80x10x4 sp=62; ISO 180/1A |
Eurostar Staramide BST44 PA6, Impact Modified, Injection Molded BST44 is a Low Temperature Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Notched (ISO) | 75.0 kJ/m² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NB40 NL IH PA6, impact modified, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 75.0 kJ/m² @Temperature -40.0 °C |
35.7 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
Solvay Specialty Polymers Amodel® EXT-1800 Polyphthalamide, extrusion
(discontinued **) AMODEL EXT-1800 was developed specifically for the extrusion process. Unlike the grades targeted for injection molding, AMODEL EXT-1800 resin can be successfully extruded into tube, pipe, sheet, fil.. |