Polymer Property : Izod Impact, Notched (ISO) = 32.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 32.0 kJ/m²

@Thickness 4.00 mm,
Temperature 23.0 °C
15.2 ft-lb/in²

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Premix Thermoplastics PRE-ELEC® PP 1392 Carbon Black Filled Conductive Thermoplastic Compound
PRE-ELEC® PP 1392 is a carbon black filled conductive thermoplastic compound based on polypropylene. In addition to a low electrical resistivity PRE-ELEC® PP 1392 has an excellent balance of mecha..
Izod Impact, Notched (ISO) 32.0 kJ/m²

@Temperature -30.0 °C
15.2 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EXRL0683 PC Copolymer
11 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched (ISO) 32.0 kJ/m²

@Temperature 23.0 °C
15.2 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Styrolution Novodur® 5300 ABS
Novodur 5300 is a high heat injection molding grade with high impact strength, good chemical resistance and reduced emission (PC modified)Information provided by Styrolution
Izod Impact, Notched (ISO) 32.0 kJ/m²

@Temperature -30.0 °C
15.2 ft-lb/in²

@Temperature -22.0 °F
ISO 180
Styron PULSEâ„¢ 2100 LG PC/ABS Engineering Resin
Overview: PULSE 2100LG Engineering Resin is designed to provide top performance in tough applications, from single piece items to intricate components. Ideal for energy management solutions, it can ..
Izod Impact, Notched (ISO) 32.0 kJ/m²

@Temperature 23.0 °C
15.2 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Borealis Daplen™ EE340AE Polypropylene TPO Compound
Daplen™ EE340AE is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q..