Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched (ISO) = 2.31 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 2.31 - 2.31 kJ/m²

@Temperature 0.000 - 0.000 °C
1.10 - 1.10 ft-lb/in²

@Temperature 32.0 - 32.0 °F
Average value: 2.31 kJ/m² Grade Count:1
Overview of materials for Chlorinated PVC (CPVC)
This property data is a summary of similar materials in the MatWeb database for the category "Chlorinated PVC (CPVC)". Each property range of values reported is minimum and maximum values of appropr..
Izod Impact, Notched (ISO) 2.31 - 2.31 kJ/m²

@Thickness 3.18 - 3.18 mm
1.10 - 1.10 ft-lb/in²

@Thickness 0.125 - 0.125 in
Average value: 2.31 kJ/m² Grade Count:1
Overview of materials for Chlorinated PVC (CPVC)
This property data is a summary of similar materials in the MatWeb database for the category "Chlorinated PVC (CPVC)". Each property range of values reported is minimum and maximum values of appropr..
Copyright © lookpolymers.com All Rights Reserved