Polymer Property : Izod Impact, Notched (ISO) = 2.09 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 4.40 kJ/m²

@Temperature -40.0 °C
2.09 ft-lb/in²

@Temperature -40.0 °F
ISO 180
Eastman Drystar 0325 Copolyester
This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen..
Izod Impact, Notched (ISO) 4.40 kJ/m²

@Temperature -40.0 °C
2.09 ft-lb/in²

@Temperature -40.0 °F
ISO 180
Eastman Drystar 0603 Copolyester
This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen..
Izod Impact, Notched (ISO) 4.40 kJ/m²

@Temperature -30.0 °C
2.09 ft-lb/in²

@Temperature -22.0 °F
ISO 180
Eastman Spectar® 14471 Copolyester
Spectar copolyester extrudes into plastic sheet that is sparkling clear, tough, chemically resistant, odor-free, versatile, easy to work with and affordable. Its toughness allows fabricators to use ..
Izod Impact, Notched (ISO) 4.40 kJ/m²

@Temperature -40.0 °C
2.09 ft-lb/in²

@Temperature -40.0 °F
ISO 180
BASF Ultramid® B3WGM24 HPX BK 2320 30% Glass/Mineral Filled PA6 (Dry)
Description: Ultramid B3WGM24 HPX BK23210 is a very high productivity, 30% glass/mineral reinforced heat stabilized injection molding PA6 grade for components that require medium rigidity, excellent..