Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 3.30 kJ/m² @Temperature -40.0 °C |
1.57 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
LyondellBasell Hifaxâ„¢ RTA3263/2 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ RTA3263/2 medium melt flow, 1,700 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good combination of rigidity, impac.. |
|||
Izod Impact, Notched (ISO) | 3.30 kJ/m² @Temperature -30.0 °C |
1.57 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
LyondellBasell Hostacomâ„¢ CB271FC Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ CB271FC high melt flow, 2,400 MPa flexural modulus, precolored, UV-stabilized, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent combination of.. |